10-Methacryloyloxydecyl Dihydrogen Phosphate (10-MDP)-Containing Cleaner Improves Bond Strength to Contaminated Monolithic Zirconia: An In-Vitro Study

Contamination of zirconia restorations before cementation can impair the resin–zirconia bonding durability. The objective of this study was to evaluate the effect of human saliva or blood decontamination with 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP)-containing cleaner on the resin–zirco...

Descripción completa

Detalles Bibliográficos
Autores principales: Awad, Mohamed M., Alhalabi, Feras, Alzahrani, Khaled Mosfer, Almutiri, Majed, Alqanawi, Fawaz, Albdiri, Lafi, Alshehri, Abdullah, Alrahlah, Ali, Ahmed, Mohammed H.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8838745/
https://www.ncbi.nlm.nih.gov/pubmed/35160968
http://dx.doi.org/10.3390/ma15031023
_version_ 1784650201300992000
author Awad, Mohamed M.
Alhalabi, Feras
Alzahrani, Khaled Mosfer
Almutiri, Majed
Alqanawi, Fawaz
Albdiri, Lafi
Alshehri, Abdullah
Alrahlah, Ali
Ahmed, Mohammed H.
author_facet Awad, Mohamed M.
Alhalabi, Feras
Alzahrani, Khaled Mosfer
Almutiri, Majed
Alqanawi, Fawaz
Albdiri, Lafi
Alshehri, Abdullah
Alrahlah, Ali
Ahmed, Mohammed H.
author_sort Awad, Mohamed M.
collection PubMed
description Contamination of zirconia restorations before cementation can impair the resin–zirconia bonding durability. The objective of this study was to evaluate the effect of human saliva or blood decontamination with 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP)-containing cleaner on the resin–zirconia shear bond strength (SBS). Methods: A total of 220 zirconia specimens were prepared and air-abraded and randomly distributed into 11 groups (n = 20 per group). Except for the control group (no contamination), zirconia specimens were contaminated with either human saliva (five groups) or blood (five groups), and then subjected to one of five cleaning methods: water rinsing, 38% phosphoric acid etchant (Pulpdent Corp., Watertown, MA, USA), 70% isopropanol alcohol (Avalon Pharma, Riyadh, Saudi Arabia), Ivoclean (Ivoclar Vivadent, Schaan, Lichtenstein) and Katana Cleaner (Kuraray Noritake, Tokyo, Japan). The resin–zirconia SBS was tested at 24 h and after thermocycling (10 k cycles). Three-way ANOVA followed by Tukey’s multiple comparisons test were utilized to analyze the SBS data. Failure modes were evaluated using a scanning electron microscope. Results: Both blood and saliva significantly affected resin–zirconia SBS as contaminants. After thermocycling, there was no statistically significant difference between SBS obtained after decontamination with the Katana Cleaner (blood, 6.026 ± 2.805 MPa; saliva, 5.206 ± 2.212 MPa) or Ivoclean (blood, 7.08 ± 3.309 MPa; saliva, 6.297 ± 3.083 MPa), and the control group (no contamination, 7.479 ± 3.64 MPa). Adhesive and mixed failures were the most frequent among the tested groups. Conclusion: Both 10-MDP-containing cleaner (Katana Cleaner) and zirconium oxide-containing cleaner (Ivoclean) could eliminate the negative effect of saliva and blood contamination on resin–zirconia SBS.
format Online
Article
Text
id pubmed-8838745
institution National Center for Biotechnology Information
language English
publishDate 2022
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-88387452022-02-13 10-Methacryloyloxydecyl Dihydrogen Phosphate (10-MDP)-Containing Cleaner Improves Bond Strength to Contaminated Monolithic Zirconia: An In-Vitro Study Awad, Mohamed M. Alhalabi, Feras Alzahrani, Khaled Mosfer Almutiri, Majed Alqanawi, Fawaz Albdiri, Lafi Alshehri, Abdullah Alrahlah, Ali Ahmed, Mohammed H. Materials (Basel) Article Contamination of zirconia restorations before cementation can impair the resin–zirconia bonding durability. The objective of this study was to evaluate the effect of human saliva or blood decontamination with 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP)-containing cleaner on the resin–zirconia shear bond strength (SBS). Methods: A total of 220 zirconia specimens were prepared and air-abraded and randomly distributed into 11 groups (n = 20 per group). Except for the control group (no contamination), zirconia specimens were contaminated with either human saliva (five groups) or blood (five groups), and then subjected to one of five cleaning methods: water rinsing, 38% phosphoric acid etchant (Pulpdent Corp., Watertown, MA, USA), 70% isopropanol alcohol (Avalon Pharma, Riyadh, Saudi Arabia), Ivoclean (Ivoclar Vivadent, Schaan, Lichtenstein) and Katana Cleaner (Kuraray Noritake, Tokyo, Japan). The resin–zirconia SBS was tested at 24 h and after thermocycling (10 k cycles). Three-way ANOVA followed by Tukey’s multiple comparisons test were utilized to analyze the SBS data. Failure modes were evaluated using a scanning electron microscope. Results: Both blood and saliva significantly affected resin–zirconia SBS as contaminants. After thermocycling, there was no statistically significant difference between SBS obtained after decontamination with the Katana Cleaner (blood, 6.026 ± 2.805 MPa; saliva, 5.206 ± 2.212 MPa) or Ivoclean (blood, 7.08 ± 3.309 MPa; saliva, 6.297 ± 3.083 MPa), and the control group (no contamination, 7.479 ± 3.64 MPa). Adhesive and mixed failures were the most frequent among the tested groups. Conclusion: Both 10-MDP-containing cleaner (Katana Cleaner) and zirconium oxide-containing cleaner (Ivoclean) could eliminate the negative effect of saliva and blood contamination on resin–zirconia SBS. MDPI 2022-01-28 /pmc/articles/PMC8838745/ /pubmed/35160968 http://dx.doi.org/10.3390/ma15031023 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Awad, Mohamed M.
Alhalabi, Feras
Alzahrani, Khaled Mosfer
Almutiri, Majed
Alqanawi, Fawaz
Albdiri, Lafi
Alshehri, Abdullah
Alrahlah, Ali
Ahmed, Mohammed H.
10-Methacryloyloxydecyl Dihydrogen Phosphate (10-MDP)-Containing Cleaner Improves Bond Strength to Contaminated Monolithic Zirconia: An In-Vitro Study
title 10-Methacryloyloxydecyl Dihydrogen Phosphate (10-MDP)-Containing Cleaner Improves Bond Strength to Contaminated Monolithic Zirconia: An In-Vitro Study
title_full 10-Methacryloyloxydecyl Dihydrogen Phosphate (10-MDP)-Containing Cleaner Improves Bond Strength to Contaminated Monolithic Zirconia: An In-Vitro Study
title_fullStr 10-Methacryloyloxydecyl Dihydrogen Phosphate (10-MDP)-Containing Cleaner Improves Bond Strength to Contaminated Monolithic Zirconia: An In-Vitro Study
title_full_unstemmed 10-Methacryloyloxydecyl Dihydrogen Phosphate (10-MDP)-Containing Cleaner Improves Bond Strength to Contaminated Monolithic Zirconia: An In-Vitro Study
title_short 10-Methacryloyloxydecyl Dihydrogen Phosphate (10-MDP)-Containing Cleaner Improves Bond Strength to Contaminated Monolithic Zirconia: An In-Vitro Study
title_sort 10-methacryloyloxydecyl dihydrogen phosphate (10-mdp)-containing cleaner improves bond strength to contaminated monolithic zirconia: an in-vitro study
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8838745/
https://www.ncbi.nlm.nih.gov/pubmed/35160968
http://dx.doi.org/10.3390/ma15031023
work_keys_str_mv AT awadmohamedm 10methacryloyloxydecyldihydrogenphosphate10mdpcontainingcleanerimprovesbondstrengthtocontaminatedmonolithiczirconiaaninvitrostudy
AT alhalabiferas 10methacryloyloxydecyldihydrogenphosphate10mdpcontainingcleanerimprovesbondstrengthtocontaminatedmonolithiczirconiaaninvitrostudy
AT alzahranikhaledmosfer 10methacryloyloxydecyldihydrogenphosphate10mdpcontainingcleanerimprovesbondstrengthtocontaminatedmonolithiczirconiaaninvitrostudy
AT almutirimajed 10methacryloyloxydecyldihydrogenphosphate10mdpcontainingcleanerimprovesbondstrengthtocontaminatedmonolithiczirconiaaninvitrostudy
AT alqanawifawaz 10methacryloyloxydecyldihydrogenphosphate10mdpcontainingcleanerimprovesbondstrengthtocontaminatedmonolithiczirconiaaninvitrostudy
AT albdirilafi 10methacryloyloxydecyldihydrogenphosphate10mdpcontainingcleanerimprovesbondstrengthtocontaminatedmonolithiczirconiaaninvitrostudy
AT alshehriabdullah 10methacryloyloxydecyldihydrogenphosphate10mdpcontainingcleanerimprovesbondstrengthtocontaminatedmonolithiczirconiaaninvitrostudy
AT alrahlahali 10methacryloyloxydecyldihydrogenphosphate10mdpcontainingcleanerimprovesbondstrengthtocontaminatedmonolithiczirconiaaninvitrostudy
AT ahmedmohammedh 10methacryloyloxydecyldihydrogenphosphate10mdpcontainingcleanerimprovesbondstrengthtocontaminatedmonolithiczirconiaaninvitrostudy