Effect of Humidity and Temperature on the Impedances and Voltage of Al/Gr-Jelly/Cu-Rubber Composite-Based Flexible Electrochemical Sensors
Here we present the fabrication of graphene and jelly (superabsorbent polymer) electrolyte composite-based shockproof flexible electrochemical sensors (Al/Gr-Jelly/Cu) and their properties under the effect of humidity and temperature. A layer of graphene mixed in jelly electrolyte was drop-casted on...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8871431/ https://www.ncbi.nlm.nih.gov/pubmed/35200455 http://dx.doi.org/10.3390/gels8020073 |
_version_ | 1784656994953592832 |
---|---|
author | Chani, Muhammad Tariq Saeed Karimov, Khasan S. Bakhsh, Esraa M. Rahman, Mohammed M. |
author_facet | Chani, Muhammad Tariq Saeed Karimov, Khasan S. Bakhsh, Esraa M. Rahman, Mohammed M. |
author_sort | Chani, Muhammad Tariq Saeed |
collection | PubMed |
description | Here we present the fabrication of graphene and jelly (superabsorbent polymer) electrolyte composite-based shockproof flexible electrochemical sensors (Al/Gr-Jelly/Cu) and their properties under the effect of humidity and temperature. A layer of graphene mixed in jelly electrolyte was drop-casted onto porous rubber substrates between preliminary fixed aluminum (Al) and copper (Cu) electrodes followed by rubbing-in. It was observed that the graphene and jelly mixture was mechanically soft and flexible, similar to jelly. Electrically, this mixture (graphene and jelly) behaved as a flexible electrolyte. It was observed that under the effect of humidity ranging from 47 to 98%, the impedances of the sensors decreased by 2.0 times on average. Under the effect of temperatures ranging from 21 to 41 °C the impedances decreased by 2.4 times. The average temperature coefficient of impedances was equal to −0.03 °C(−1). The electrochemical voltage generated by the flexible jelly electrolyte sensors was also investigated. It was found that the initial open-circuit voltages were equal to 201 mV and increased slightly, by 5–10% under the effect of humidity and temperature as well. The short-circuit currents under the effect of humidity and temperature increased by 2–3 times. The Al/Gr-Jelly/Cu electrochemical sensors may be used as prototypes for the development of the jelly electronic-based devices. |
format | Online Article Text |
id | pubmed-8871431 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2022 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-88714312022-02-25 Effect of Humidity and Temperature on the Impedances and Voltage of Al/Gr-Jelly/Cu-Rubber Composite-Based Flexible Electrochemical Sensors Chani, Muhammad Tariq Saeed Karimov, Khasan S. Bakhsh, Esraa M. Rahman, Mohammed M. Gels Article Here we present the fabrication of graphene and jelly (superabsorbent polymer) electrolyte composite-based shockproof flexible electrochemical sensors (Al/Gr-Jelly/Cu) and their properties under the effect of humidity and temperature. A layer of graphene mixed in jelly electrolyte was drop-casted onto porous rubber substrates between preliminary fixed aluminum (Al) and copper (Cu) electrodes followed by rubbing-in. It was observed that the graphene and jelly mixture was mechanically soft and flexible, similar to jelly. Electrically, this mixture (graphene and jelly) behaved as a flexible electrolyte. It was observed that under the effect of humidity ranging from 47 to 98%, the impedances of the sensors decreased by 2.0 times on average. Under the effect of temperatures ranging from 21 to 41 °C the impedances decreased by 2.4 times. The average temperature coefficient of impedances was equal to −0.03 °C(−1). The electrochemical voltage generated by the flexible jelly electrolyte sensors was also investigated. It was found that the initial open-circuit voltages were equal to 201 mV and increased slightly, by 5–10% under the effect of humidity and temperature as well. The short-circuit currents under the effect of humidity and temperature increased by 2–3 times. The Al/Gr-Jelly/Cu electrochemical sensors may be used as prototypes for the development of the jelly electronic-based devices. MDPI 2022-01-24 /pmc/articles/PMC8871431/ /pubmed/35200455 http://dx.doi.org/10.3390/gels8020073 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Chani, Muhammad Tariq Saeed Karimov, Khasan S. Bakhsh, Esraa M. Rahman, Mohammed M. Effect of Humidity and Temperature on the Impedances and Voltage of Al/Gr-Jelly/Cu-Rubber Composite-Based Flexible Electrochemical Sensors |
title | Effect of Humidity and Temperature on the Impedances and Voltage of Al/Gr-Jelly/Cu-Rubber Composite-Based Flexible Electrochemical Sensors |
title_full | Effect of Humidity and Temperature on the Impedances and Voltage of Al/Gr-Jelly/Cu-Rubber Composite-Based Flexible Electrochemical Sensors |
title_fullStr | Effect of Humidity and Temperature on the Impedances and Voltage of Al/Gr-Jelly/Cu-Rubber Composite-Based Flexible Electrochemical Sensors |
title_full_unstemmed | Effect of Humidity and Temperature on the Impedances and Voltage of Al/Gr-Jelly/Cu-Rubber Composite-Based Flexible Electrochemical Sensors |
title_short | Effect of Humidity and Temperature on the Impedances and Voltage of Al/Gr-Jelly/Cu-Rubber Composite-Based Flexible Electrochemical Sensors |
title_sort | effect of humidity and temperature on the impedances and voltage of al/gr-jelly/cu-rubber composite-based flexible electrochemical sensors |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8871431/ https://www.ncbi.nlm.nih.gov/pubmed/35200455 http://dx.doi.org/10.3390/gels8020073 |
work_keys_str_mv | AT chanimuhammadtariqsaeed effectofhumidityandtemperatureontheimpedancesandvoltageofalgrjellycurubbercompositebasedflexibleelectrochemicalsensors AT karimovkhasans effectofhumidityandtemperatureontheimpedancesandvoltageofalgrjellycurubbercompositebasedflexibleelectrochemicalsensors AT bakhshesraam effectofhumidityandtemperatureontheimpedancesandvoltageofalgrjellycurubbercompositebasedflexibleelectrochemicalsensors AT rahmanmohammedm effectofhumidityandtemperatureontheimpedancesandvoltageofalgrjellycurubbercompositebasedflexibleelectrochemicalsensors |