Cargando…

Influence of the Pyrolysis Temperature and TiO(2)-Incorporation on the Properties of SiOC/SiC Composites for Efficient Wastewater Treatment Applications

This study focuses on the development of porous ceramer and SiOC composites which are suitable for microfiltration applications, using a mixture of polysiloxanes as the preceramic precursor. The properties of the membranes—such as their pore size, hydrophilicity, specific surface area, and mechanica...

Descripción completa

Detalles Bibliográficos
Autores principales: Fontão, Natália C., Ferrari, Lucas N., Sapatieri, Joice C., Rezwan, Kurosch, Wilhelm, Michaela
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8875749/
https://www.ncbi.nlm.nih.gov/pubmed/35207096
http://dx.doi.org/10.3390/membranes12020175
Descripción
Sumario:This study focuses on the development of porous ceramer and SiOC composites which are suitable for microfiltration applications, using a mixture of polysiloxanes as the preceramic precursor. The properties of the membranes—such as their pore size, hydrophilicity, specific surface area, and mechanical resistance—were tailored in a one-step process, according to the choice of pyrolysis temperatures (600–1000 °C) and the incorporation of micro- (SiC) and nanofillers (TiO(2)). Lower pyrolysis temperatures (<700 °C) allowed the incorporation of TiO(2) in its photocatalytically active anatase phase, enabling the study of its photocatalytic decomposition. The produced materials showed low photocatalytic activity; however, a high adsorption capacity for methylene blue was observed, which could be suitable for dye-removal applications. The membrane performance was evaluated in terms of its maximum flexural strength, water permeation, and separation of an oil-in-water emulsion. The mechanical resistance increased with an increase of the pyrolysis temperature, as the preceramic precursor underwent the ceramization process. Water fluxes varying from 2.5 to 370 L/m(2)·h (2 bar) were obtained according to the membrane pore sizes and surface characteristics. Oil-rejection ratios of 81–98% were obtained at an initial oil concentration of 1000 mg/L, indicating a potential application of the produced PDC membranes in the treatment of oily wastewater.