Organosolv Lignin Improved Thermoplastic Elastomeric Behavior of Polyethylene/Polyisoprene Blend

[Image: see text] Thermoplastic elastomers are considered the fastest-growing elastomers in recent years because of their thermomechanical recyclability, in contrast to traditional thermoset rubbers. Polyolefins such as low-density polyethylene (LDPE) show low mechanical properties, particularly poo...

Descripción completa

Detalles Bibliográficos
Autor principal: Ghosh, Arun
Formato: Online Artículo Texto
Lenguaje:English
Publicado: American Chemical Society 2022
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8928528/
https://www.ncbi.nlm.nih.gov/pubmed/35309423
http://dx.doi.org/10.1021/acsomega.1c06062
_version_ 1784670661317230592
author Ghosh, Arun
author_facet Ghosh, Arun
author_sort Ghosh, Arun
collection PubMed
description [Image: see text] Thermoplastic elastomers are considered the fastest-growing elastomers in recent years because of their thermomechanical recyclability, in contrast to traditional thermoset rubbers. Polyolefins such as low-density polyethylene (LDPE) show low mechanical properties, particularly poor elongation when compared with an elastomer or rubber. In this study, LDPE resin is converted to highly ductile rubber-like materials with high elongation and low modulus properties on blending with polyisoprene rubber (IR), followed by treating with dicumyl peroxide as a curing agent and organosolv lignin as an additive. The technique of high shear melt-mixing, in conjunction with vulcanization or crosslinking using organic peroxide, is used to develop hybrid materials based on the LDPE/IR blend at a 70/30 mass ratio, where LDPE is replaced partly with lignin. Various characteristics such as tensile, viscoelasticity, melt flow, crystallinity, and phase morphology of the materials are analyzed. As expected, vulcanization with peroxide can improve the mechanical performance of the LDPE/IR blends, which is further improved with the application of lignin (2 to 5 wt. %), particularly tensile strain is profoundly increased. For example, the average values of the tensile strength, the modulus, and the ultimate elongation of neat LDPE resin are 7.8 MPa, 177 MPa, and 62%, respectively, and those of LDPE/IR/lignin/DCP 65/30/05/2 are 8.1 MPa, 95 MPa, and 238%, respectively. It indicates that the application of lignin/DCP has a profound effect on improving the ductility and elastomeric characteristics of the materials; thus, this material can have the potential to replace traditional rubber products.
format Online
Article
Text
id pubmed-8928528
institution National Center for Biotechnology Information
language English
publishDate 2022
publisher American Chemical Society
record_format MEDLINE/PubMed
spelling pubmed-89285282022-03-18 Organosolv Lignin Improved Thermoplastic Elastomeric Behavior of Polyethylene/Polyisoprene Blend Ghosh, Arun ACS Omega [Image: see text] Thermoplastic elastomers are considered the fastest-growing elastomers in recent years because of their thermomechanical recyclability, in contrast to traditional thermoset rubbers. Polyolefins such as low-density polyethylene (LDPE) show low mechanical properties, particularly poor elongation when compared with an elastomer or rubber. In this study, LDPE resin is converted to highly ductile rubber-like materials with high elongation and low modulus properties on blending with polyisoprene rubber (IR), followed by treating with dicumyl peroxide as a curing agent and organosolv lignin as an additive. The technique of high shear melt-mixing, in conjunction with vulcanization or crosslinking using organic peroxide, is used to develop hybrid materials based on the LDPE/IR blend at a 70/30 mass ratio, where LDPE is replaced partly with lignin. Various characteristics such as tensile, viscoelasticity, melt flow, crystallinity, and phase morphology of the materials are analyzed. As expected, vulcanization with peroxide can improve the mechanical performance of the LDPE/IR blends, which is further improved with the application of lignin (2 to 5 wt. %), particularly tensile strain is profoundly increased. For example, the average values of the tensile strength, the modulus, and the ultimate elongation of neat LDPE resin are 7.8 MPa, 177 MPa, and 62%, respectively, and those of LDPE/IR/lignin/DCP 65/30/05/2 are 8.1 MPa, 95 MPa, and 238%, respectively. It indicates that the application of lignin/DCP has a profound effect on improving the ductility and elastomeric characteristics of the materials; thus, this material can have the potential to replace traditional rubber products. American Chemical Society 2022-03-01 /pmc/articles/PMC8928528/ /pubmed/35309423 http://dx.doi.org/10.1021/acsomega.1c06062 Text en © 2022 The Author. Published by American Chemical Society https://creativecommons.org/licenses/by/4.0/Permits the broadest form of re-use including for commercial purposes, provided that author attribution and integrity are maintained (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Ghosh, Arun
Organosolv Lignin Improved Thermoplastic Elastomeric Behavior of Polyethylene/Polyisoprene Blend
title Organosolv Lignin Improved Thermoplastic Elastomeric Behavior of Polyethylene/Polyisoprene Blend
title_full Organosolv Lignin Improved Thermoplastic Elastomeric Behavior of Polyethylene/Polyisoprene Blend
title_fullStr Organosolv Lignin Improved Thermoplastic Elastomeric Behavior of Polyethylene/Polyisoprene Blend
title_full_unstemmed Organosolv Lignin Improved Thermoplastic Elastomeric Behavior of Polyethylene/Polyisoprene Blend
title_short Organosolv Lignin Improved Thermoplastic Elastomeric Behavior of Polyethylene/Polyisoprene Blend
title_sort organosolv lignin improved thermoplastic elastomeric behavior of polyethylene/polyisoprene blend
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8928528/
https://www.ncbi.nlm.nih.gov/pubmed/35309423
http://dx.doi.org/10.1021/acsomega.1c06062
work_keys_str_mv AT ghosharun organosolvligninimprovedthermoplasticelastomericbehaviorofpolyethylenepolyisopreneblend