Building Ultra-Stable and Low-Polarization Composite Zn Anode Interface via Hydrated Polyzwitterionic Electrolyte Construction
Aqueous zinc metal batteries are noted for their cost-effectiveness, safety and environmental friendliness. However, the water-induced notorious issues such as continuous electrolyte decomposition and uneven Zn electrochemical deposition remarkably restrict the development of the long-life zinc meta...
Autores principales: | , , , , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Springer Nature Singapore
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8986915/ https://www.ncbi.nlm.nih.gov/pubmed/35384517 http://dx.doi.org/10.1007/s40820-022-00835-3 |
_version_ | 1784682628415225856 |
---|---|
author | He, Qiong Fang, Guozhao Chang, Zhi Zhang, Yifang Zhou, Shuang Zhou, Miao Chai, Simin Zhong, Yue Cao, Guozhong Liang, Shuquan Pan, Anqiang |
author_facet | He, Qiong Fang, Guozhao Chang, Zhi Zhang, Yifang Zhou, Shuang Zhou, Miao Chai, Simin Zhong, Yue Cao, Guozhong Liang, Shuquan Pan, Anqiang |
author_sort | He, Qiong |
collection | PubMed |
description | Aqueous zinc metal batteries are noted for their cost-effectiveness, safety and environmental friendliness. However, the water-induced notorious issues such as continuous electrolyte decomposition and uneven Zn electrochemical deposition remarkably restrict the development of the long-life zinc metal batteries. In this study, zwitterionic sulfobetaine is introduced to copolymerize with acrylamide in zinc perchlorate (Zn(ClO(4))(2)) solution. The designed gel framework with hydrophilic and charged groups can firmly anchor water molecules and construct ion migration channels to accelerate ion transport. The in situ generated hybrid interface, which is composed of the organic functionalized outer layer and inorganic Cl(−) containing inner layer, can synergically lower the mass transfer overpotential, reduce water-related side reactions and lead to uniform Zn deposition. Such a novel electrolyte configuration enables Zn//Zn cells with an ultra-long cycling life of over 3000 h and a low polarization potential (~ 0.03 V) and Zn//Cu cells with high Coulombic efficiency of 99.18% for 1000 cycles. Full cells matched with MnO(2) cathodes delivered laudable cycling stability and impressive shelving ability. Besides, the flexible quasi-solid-state batteries which are equipped with the anti-vandalism ability (such as cutting, hammering and soaking) can successfully power the LED simultaneously. Such a safe, processable and durable hydrogel promises significant application potential for long-life flexible electronic devices. [Image: see text] SUPPLEMENTARY INFORMATION: The online version contains supplementary material available at 10.1007/s40820-022-00835-3. |
format | Online Article Text |
id | pubmed-8986915 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2022 |
publisher | Springer Nature Singapore |
record_format | MEDLINE/PubMed |
spelling | pubmed-89869152022-04-22 Building Ultra-Stable and Low-Polarization Composite Zn Anode Interface via Hydrated Polyzwitterionic Electrolyte Construction He, Qiong Fang, Guozhao Chang, Zhi Zhang, Yifang Zhou, Shuang Zhou, Miao Chai, Simin Zhong, Yue Cao, Guozhong Liang, Shuquan Pan, Anqiang Nanomicro Lett Article Aqueous zinc metal batteries are noted for their cost-effectiveness, safety and environmental friendliness. However, the water-induced notorious issues such as continuous electrolyte decomposition and uneven Zn electrochemical deposition remarkably restrict the development of the long-life zinc metal batteries. In this study, zwitterionic sulfobetaine is introduced to copolymerize with acrylamide in zinc perchlorate (Zn(ClO(4))(2)) solution. The designed gel framework with hydrophilic and charged groups can firmly anchor water molecules and construct ion migration channels to accelerate ion transport. The in situ generated hybrid interface, which is composed of the organic functionalized outer layer and inorganic Cl(−) containing inner layer, can synergically lower the mass transfer overpotential, reduce water-related side reactions and lead to uniform Zn deposition. Such a novel electrolyte configuration enables Zn//Zn cells with an ultra-long cycling life of over 3000 h and a low polarization potential (~ 0.03 V) and Zn//Cu cells with high Coulombic efficiency of 99.18% for 1000 cycles. Full cells matched with MnO(2) cathodes delivered laudable cycling stability and impressive shelving ability. Besides, the flexible quasi-solid-state batteries which are equipped with the anti-vandalism ability (such as cutting, hammering and soaking) can successfully power the LED simultaneously. Such a safe, processable and durable hydrogel promises significant application potential for long-life flexible electronic devices. [Image: see text] SUPPLEMENTARY INFORMATION: The online version contains supplementary material available at 10.1007/s40820-022-00835-3. Springer Nature Singapore 2022-04-06 /pmc/articles/PMC8986915/ /pubmed/35384517 http://dx.doi.org/10.1007/s40820-022-00835-3 Text en © The Author(s) 2022 https://creativecommons.org/licenses/by/4.0/Open AccessThis article is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons licence, and indicate if changes were made. The images or other third party material in this article are included in the article's Creative Commons licence, unless indicated otherwise in a credit line to the material. If material is not included in the article's Creative Commons licence and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder. To view a copy of this licence, visit http://creativecommons.org/licenses/by/4.0/ (https://creativecommons.org/licenses/by/4.0/) . |
spellingShingle | Article He, Qiong Fang, Guozhao Chang, Zhi Zhang, Yifang Zhou, Shuang Zhou, Miao Chai, Simin Zhong, Yue Cao, Guozhong Liang, Shuquan Pan, Anqiang Building Ultra-Stable and Low-Polarization Composite Zn Anode Interface via Hydrated Polyzwitterionic Electrolyte Construction |
title | Building Ultra-Stable and Low-Polarization Composite Zn Anode Interface via Hydrated Polyzwitterionic Electrolyte Construction |
title_full | Building Ultra-Stable and Low-Polarization Composite Zn Anode Interface via Hydrated Polyzwitterionic Electrolyte Construction |
title_fullStr | Building Ultra-Stable and Low-Polarization Composite Zn Anode Interface via Hydrated Polyzwitterionic Electrolyte Construction |
title_full_unstemmed | Building Ultra-Stable and Low-Polarization Composite Zn Anode Interface via Hydrated Polyzwitterionic Electrolyte Construction |
title_short | Building Ultra-Stable and Low-Polarization Composite Zn Anode Interface via Hydrated Polyzwitterionic Electrolyte Construction |
title_sort | building ultra-stable and low-polarization composite zn anode interface via hydrated polyzwitterionic electrolyte construction |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8986915/ https://www.ncbi.nlm.nih.gov/pubmed/35384517 http://dx.doi.org/10.1007/s40820-022-00835-3 |
work_keys_str_mv | AT heqiong buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT fangguozhao buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT changzhi buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT zhangyifang buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT zhoushuang buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT zhoumiao buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT chaisimin buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT zhongyue buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT caoguozhong buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT liangshuquan buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction AT pananqiang buildingultrastableandlowpolarizationcompositeznanodeinterfaceviahydratedpolyzwitterionicelectrolyteconstruction |