Mechanical Behavior of Alkasite Posterior Restorations in Comparison to Polymeric Materials: A 3D-FEA Study
The present investigation evaluated the effect of the combination of different dental filling materials in Class I cavities under occlusal loading using three-dimensional finite elements analysis (FEA). Six computer-generated and restored models of a lower molar were created in the CAD software and...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9024758/ https://www.ncbi.nlm.nih.gov/pubmed/35458251 http://dx.doi.org/10.3390/polym14081502 |
Sumario: | The present investigation evaluated the effect of the combination of different dental filling materials in Class I cavities under occlusal loading using three-dimensional finite elements analysis (FEA). Six computer-generated and restored models of a lower molar were created in the CAD software and compared according to the biomechanical response during chewing load condition. Two adhesively bonded bulk restorative materials [bulk-fill resin composite (BF) or Alkasite (Alk)] were evaluated with or without the presence of a base material below (flowable resin composite or glass ionomer cement). A food bolus was placed on the occlusal surface mimicking the compressive occlusal load (600 N) during the static linear analysis. The maximum principal stress (tensile) was calculated as stress criteria in enamel, dentin and restoration. All models showed high stresses along the enamel/restoration margin with a similar stress trend for models restored with the same upper-layer material. Stress values up to 12.04 MPa (Alk) or up to 11.12 MPa (BF) were recorded at the enamel margins. The use of flexible polymeric or ionic base material in combination with bulk-fill resin composite or Alk did not reduce the stress magnitude in dentine and enamel. Class I cavities adhesively restored with bulk-fill resin composite showed lighter stress concentration as well as Alk. Therefore, adhesively bonded Alk restoration showed a promising mechanical behavior when used with different base materials or as a bulk restoration for posterior Class I cavity. |
---|