Electrochemical Performance of Carbon-Rich Silicon Carbonitride Ceramic as Support for Sulfur Cathode in Lithium Sulfur Battery
As a promising matrix material for anchoring sulfur in the cathode for lithium-sulfur (Li-S) batteries, porous conducting supports have gained much attention. In this work, sulfur-containing C-rich SiCN composites are processed from silicon carbonitride (SiCN) ceramics, synthesized at temperatures f...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9031311/ https://www.ncbi.nlm.nih.gov/pubmed/35457991 http://dx.doi.org/10.3390/nano12081283 |
Sumario: | As a promising matrix material for anchoring sulfur in the cathode for lithium-sulfur (Li-S) batteries, porous conducting supports have gained much attention. In this work, sulfur-containing C-rich SiCN composites are processed from silicon carbonitride (SiCN) ceramics, synthesized at temperatures from 800 to 1100 °C. To embed sulfur in the porous SiCN matrix, an easy and scalable procedure, denoted as melting-diffusion method, is applied. Accordingly, sulfur is infiltrated under solvothermal conditions at 155 °C into pores of carbon-rich silicon carbonitride (C-rich SiCN). The impact of the initial porosity and microstructure of the SiCN ceramics on the electrochemical performance of the synthesized SiCN-sulfur (SiCN-S) composites is analysed and discussed. A combination of the mesoporous character of SiCN and presence of a disordered free carbon phase makes the electrochemical performance of the SiCN matrix obtained at 900 °C superior to that of SiCN synthesized at lower and higher temperatures. A capacity value of more than 195 mAh/g over 50 cycles at a high sulfur content of 66 wt.% is achieved. |
---|