Calcium carbonate modified urea–formaldehyde resin adhesive for strength enhanced medium density fiberboard production

This study investigated the improved properties of calcium carbonate (CaCO(3)) modified urea–formaldehyde (UF) resin adhesive for medium density fiberboard (MDF) production. The CaCO(3) modified UF resins were prepared by adding different proportions of CaCO(3) to a low molar ratio UF resin at the i...

Descripción completa

Detalles Bibliográficos
Autores principales: Lu, Li, Wang, Yan, Li, Tianhua, Wang, Supeng, Yang, Shoulu, Qing, Yan, Li, Xingong, Wu, Yiqiang, Liu, Ming
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Royal Society of Chemistry 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9036895/
https://www.ncbi.nlm.nih.gov/pubmed/35481052
http://dx.doi.org/10.1039/d1ra04316a
_version_ 1784693613997850624
author Lu, Li
Wang, Yan
Li, Tianhua
Wang, Supeng
Yang, Shoulu
Qing, Yan
Li, Xingong
Wu, Yiqiang
Liu, Ming
author_facet Lu, Li
Wang, Yan
Li, Tianhua
Wang, Supeng
Yang, Shoulu
Qing, Yan
Li, Xingong
Wu, Yiqiang
Liu, Ming
author_sort Lu, Li
collection PubMed
description This study investigated the improved properties of calcium carbonate (CaCO(3)) modified urea–formaldehyde (UF) resin adhesive for medium density fiberboard (MDF) production. The CaCO(3) modified UF resins were prepared by adding different proportions of CaCO(3) to a low molar ratio UF resin at the initial stage of a typical synthetic process of the resin. The physicochemical properties of the resins were measured. The mechanical and environmental performances of the resin-bonded MDF panels were tested. The results show that the viscosity and free formaldehyde content of UF resins with or without CaCO(3) modification were not significantly different. The solid content of the CaCO(3) modified UF resin was significantly lower than that of the control group. In addition, the measured gel time of the CaCO(3) modified UF resin was 111–149 s, which was longer than that of the control resin (82 s). The gel time was further extended with the increase of the CaCO(3) content in the UF resin. The chemical group and crystal structure of UF resins with or without the modification of CaCO(3) were not significantly different. The internal bonding (IB) strength of the MDF panels significantly increased from 0.75 MPa to 0.97 MPa when the UF resin was modified with 2% of CaCO(3). This study provides scientific support for the preparation of inorganic mineral modified UF resins for strength enhanced wood-based panel manufacturing.
format Online
Article
Text
id pubmed-9036895
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher The Royal Society of Chemistry
record_format MEDLINE/PubMed
spelling pubmed-90368952022-04-26 Calcium carbonate modified urea–formaldehyde resin adhesive for strength enhanced medium density fiberboard production Lu, Li Wang, Yan Li, Tianhua Wang, Supeng Yang, Shoulu Qing, Yan Li, Xingong Wu, Yiqiang Liu, Ming RSC Adv Chemistry This study investigated the improved properties of calcium carbonate (CaCO(3)) modified urea–formaldehyde (UF) resin adhesive for medium density fiberboard (MDF) production. The CaCO(3) modified UF resins were prepared by adding different proportions of CaCO(3) to a low molar ratio UF resin at the initial stage of a typical synthetic process of the resin. The physicochemical properties of the resins were measured. The mechanical and environmental performances of the resin-bonded MDF panels were tested. The results show that the viscosity and free formaldehyde content of UF resins with or without CaCO(3) modification were not significantly different. The solid content of the CaCO(3) modified UF resin was significantly lower than that of the control group. In addition, the measured gel time of the CaCO(3) modified UF resin was 111–149 s, which was longer than that of the control resin (82 s). The gel time was further extended with the increase of the CaCO(3) content in the UF resin. The chemical group and crystal structure of UF resins with or without the modification of CaCO(3) were not significantly different. The internal bonding (IB) strength of the MDF panels significantly increased from 0.75 MPa to 0.97 MPa when the UF resin was modified with 2% of CaCO(3). This study provides scientific support for the preparation of inorganic mineral modified UF resins for strength enhanced wood-based panel manufacturing. The Royal Society of Chemistry 2021-07-19 /pmc/articles/PMC9036895/ /pubmed/35481052 http://dx.doi.org/10.1039/d1ra04316a Text en This journal is © The Royal Society of Chemistry https://creativecommons.org/licenses/by-nc/3.0/
spellingShingle Chemistry
Lu, Li
Wang, Yan
Li, Tianhua
Wang, Supeng
Yang, Shoulu
Qing, Yan
Li, Xingong
Wu, Yiqiang
Liu, Ming
Calcium carbonate modified urea–formaldehyde resin adhesive for strength enhanced medium density fiberboard production
title Calcium carbonate modified urea–formaldehyde resin adhesive for strength enhanced medium density fiberboard production
title_full Calcium carbonate modified urea–formaldehyde resin adhesive for strength enhanced medium density fiberboard production
title_fullStr Calcium carbonate modified urea–formaldehyde resin adhesive for strength enhanced medium density fiberboard production
title_full_unstemmed Calcium carbonate modified urea–formaldehyde resin adhesive for strength enhanced medium density fiberboard production
title_short Calcium carbonate modified urea–formaldehyde resin adhesive for strength enhanced medium density fiberboard production
title_sort calcium carbonate modified urea–formaldehyde resin adhesive for strength enhanced medium density fiberboard production
topic Chemistry
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9036895/
https://www.ncbi.nlm.nih.gov/pubmed/35481052
http://dx.doi.org/10.1039/d1ra04316a
work_keys_str_mv AT luli calciumcarbonatemodifiedureaformaldehyderesinadhesiveforstrengthenhancedmediumdensityfiberboardproduction
AT wangyan calciumcarbonatemodifiedureaformaldehyderesinadhesiveforstrengthenhancedmediumdensityfiberboardproduction
AT litianhua calciumcarbonatemodifiedureaformaldehyderesinadhesiveforstrengthenhancedmediumdensityfiberboardproduction
AT wangsupeng calciumcarbonatemodifiedureaformaldehyderesinadhesiveforstrengthenhancedmediumdensityfiberboardproduction
AT yangshoulu calciumcarbonatemodifiedureaformaldehyderesinadhesiveforstrengthenhancedmediumdensityfiberboardproduction
AT qingyan calciumcarbonatemodifiedureaformaldehyderesinadhesiveforstrengthenhancedmediumdensityfiberboardproduction
AT lixingong calciumcarbonatemodifiedureaformaldehyderesinadhesiveforstrengthenhancedmediumdensityfiberboardproduction
AT wuyiqiang calciumcarbonatemodifiedureaformaldehyderesinadhesiveforstrengthenhancedmediumdensityfiberboardproduction
AT liuming calciumcarbonatemodifiedureaformaldehyderesinadhesiveforstrengthenhancedmediumdensityfiberboardproduction