Which fraction of stone wool fibre surface remains uncoated by binder? A detailed analysis by time-of-flight secondary ion mass spectrometry and X-ray photoelectron spectroscopy
Biodurability of man-made vitreous fibres (MMVF) is often measured on naked fibres, i.e. fibres devoid of the phenol-urea-formaldehyde (PUF) binder that is sprayed and baked on the commercial product to reduce dustiness and to provide mechanical strength to fibre mats. This simplification of the haz...
Autores principales: | Hirth, Sabine, Waindok, Hubert, Wohlleben, Wendel |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Royal Society of Chemistry
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9044424/ https://www.ncbi.nlm.nih.gov/pubmed/35492464 http://dx.doi.org/10.1039/d1ra06251d |
Ejemplares similares
-
Reply to comment on “which fraction of stone wool fibre surface remains uncoated by binder? A detailed analysis by time-of-flight secondary ion mass spectrometry and X-ray photoelectron spectroscopy” by Hirth et al., 2021, RSC Adv., 11, 39545, DOI: 10.1039/d1ra06251d”
por: Hirth, Sabine, et al.
Publicado: (2023) -
Composition, Respirable Fraction and Dissolution Rate of 24 Stone Wool MMVF with their Binder
por: Wohlleben, Wendel, et al.
Publicado: (2017) -
Comment on “Which fraction of stone wool fibre surface remains uncoated by binder? A detailed analysis by time-of-flight secondary ion mass spectrometry and X-ray photoelectron spectroscopy” by Hirth et al., 2021, RSC Adv., 11, 39545, DOI: 10.1039/d1ra06251d
por: Okhrimenko, Denis V., et al.
Publicado: (2023) -
Gelatin–Tannin-Based Greener Binder Technology
for Stone Shot and Stone Wool Materials: A Detailed Study
por: Hjelmgaard, Thomas, et al.
Publicado: (2021) -
Picornavirus uncoating intermediate captured in atomic detail
por: Ren, Jingshan, et al.
Publicado: (2013)