Mechanism and kinetics of magnetite oxidation under hydrothermal conditions
The stability of magnetite under oxidizing hydrothermal conditions was evaluated at temperatures of 120, 150, 180 and 275 °C. A well-characterized sample of commercially-available magnetite with a particle size of approximately 690 nm was oxidized by dissolved oxygen (DO) under alkaline hydrothermal...
Autores principales: | Li, Zimin, Chanéac, Corinne, Berger, Gilles, Delaunay, Sophie, Graff, Anaïs, Lefèvre, Grégory |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Royal Society of Chemistry
2019
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9073545/ https://www.ncbi.nlm.nih.gov/pubmed/35528876 http://dx.doi.org/10.1039/c9ra03234g |
Ejemplares similares
-
Anaerobic oxidation of aldehydes to carboxylic acids under hydrothermal conditions
por: Liao, Yiju, et al.
Publicado: (2022) -
Correction: Anaerobic oxidation of aldehydes to carboxylic acids under hydrothermal conditions
por: Liao, Yiju, et al.
Publicado: (2023) -
Hydrothermal phase transformation of hematite to magnetite
por: Lu, Jie-feng, et al.
Publicado: (2014) -
Potential application of carbohydrate biomass in hydrometallurgy: one-pot reduction of metal oxides/salts under mild hydrothermal conditions
por: Zhou, Yangyuan, et al.
Publicado: (2022) -
Retraction: Equilibrium and kinetic studies on adsorptive removal of malachite green by the citrate-stabilized magnetite nanoparticles
por: Fisher, Laura
Publicado: (2020)