Cargando…
Effect of extremely high CO(2) pressure on the formation of the corrosion film on 13Cr stainless steel
The corrosion behaviors of 13Cr martensitic steel under different CO(2) partial pressures (4–28 MPa) were investigated by weight loss tests and surface characterizations. The results show that the corrosion rate of 13Cr steel shows a sharp increase under higher CO(2) pressure (28 MPa), which reached...
Autores principales: | Zhu, Jinyang, Li, Dapeng, Zhang, Yunan, Zhang, Lei |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Royal Society of Chemistry
2019
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9076110/ https://www.ncbi.nlm.nih.gov/pubmed/35540226 http://dx.doi.org/10.1039/c9ra08373a |
Ejemplares similares
-
Effect of chromium on the corrosion behaviour of low Cr-bearing alloy steel under an extremely high flow rate
por: Wang, Bei, et al.
Publicado: (2020) -
Corrosion of stainless steels /
por: Sedriks, A. John
Publicado: (1996) -
Corrosion of stainless steels
por: Sedriks, A John
Publicado: (1996) -
Modeling Corrosion Product Film Formation and Hydrogen Diffusion at the Crack Tip of Austenitic Stainless Steel
por: Yang, Fuqiang, et al.
Publicado: (2023) -
Fundamental aspects of the corrosion of N80 steel in a formation water system under high CO(2) partial pressure at 100 °C
por: Li, Huixin, et al.
Publicado: (2019)