Degradation of OLED performance by exposure to UV irradiation
Organic light-emitting diode (OLED) displays are highly susceptible to the harsh environmental conditions found outdoors, like exposure to direct sunlight as well as UV radiation and storage temperature, resulting in a loss of luminance and lifespan, pixel shrinkage, and permanent damage and/or malf...
Autores principales: | Kwon, Sun-Kap, Baek, Ji-Ho, Choi, Hyun-Chul, Kim, Seong Keun, Lampande, Raju, Pode, Ramchandra, Kwon, Jang Hyuk |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Royal Society of Chemistry
2019
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9076695/ https://www.ncbi.nlm.nih.gov/pubmed/35542867 http://dx.doi.org/10.1039/c9ra09730a |
Ejemplares similares
-
An efficient organic and inorganic hybrid interlayer for high performance inverted red cadmium-free quantum dot light-emitting diodes
por: Mude, Nagarjuna Naik, et al.
Publicado: (2021) -
Recent Advancement in Boron-Based Efficient and Pure Blue Thermally Activated Delayed Fluorescence Materials for Organic Light-Emitting Diodes
por: Lee, Hyuna, et al.
Publicado: (2020) -
Highly efficient single-stack hybrid cool white OLED utilizing blue thermally activated delayed fluorescent and yellow phosphorescent emitters
por: Kim, Gyeong Woo, et al.
Publicado: (2018) -
δ-Carboline-based bipolar host materials for deep blue thermally activated delayed fluorescence OLEDs with high efficiency and low roll-off characteristic
por: Moon, Ji Su, et al.
Publicado: (2018) -
Identification of OLED Degradation Scenarios by Kinetic Monte Carlo Simulations of Lifetime Experiments
por: Hauenstein, Christoph, et al.
Publicado: (2022)