Cargando…
A new mechanism for improving electromagnetic properties based on tunable crystallographic structures of FeCoNiSi(x)Al(0.4) high entropy alloy powders
Mechanical grinding method was employed to prepare FeCoNiSi(x)Al(0.4) high entropy alloy powders, which present a simple solid solution structure (FCC and BCC). After annealing at 673 K, a large amount of BCC phase precipitate and a small amount of CoFe(2)O(4) phase generate. The change of crystal s...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Royal Society of Chemistry
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9079992/ https://www.ncbi.nlm.nih.gov/pubmed/35541311 http://dx.doi.org/10.1039/c8ra01762j |
_version_ | 1784702682799276032 |
---|---|
author | Zhang, Bin Duan, Yuping Cui, Yulong Ma, Guojia Wang, Tongmin Dong, Xinglong |
author_facet | Zhang, Bin Duan, Yuping Cui, Yulong Ma, Guojia Wang, Tongmin Dong, Xinglong |
author_sort | Zhang, Bin |
collection | PubMed |
description | Mechanical grinding method was employed to prepare FeCoNiSi(x)Al(0.4) high entropy alloy powders, which present a simple solid solution structure (FCC and BCC). After annealing at 673 K, a large amount of BCC phase precipitate and a small amount of CoFe(2)O(4) phase generate. The change of crystal structure may lead to an increase in M(s) (from 100.3 emu g(−1) to 124.2 emu g(−1)) and a decrease in H(c) (from 107 Oe to 59.5 Oe for FeCoNiSi(0.3)Al(0.4)). The silica content has a significant effect on the electromagnetic parameters of the as-milled and as-annealed alloy powders, presenting the trend of first increase and then decrease. And the dielectric constant is obviously improved after annealing (e.g. from 8.48 to 11.21 and from 0.15 to 2.84 for the ε′ and ε′′ of FeCoNiSi(0.3)Al(0.4) at 18 GHz, respectively), while the permeability is reduced. Compared with those of the as-milled samples, the μ′ of as-annealed FeCoNiSi(x)Al(0.4) (x = 0.1, 0.3, 0.4) remain unchanged or even increase due to the formation of CoFe(2)O(4). Meanwhile, the relative content of the precipitated BCC to FCC for FeCoNiSi(0.3)Al(0.4) enhance with the annealing temperature increase from 573 K to 773 K, and then reduce. And the ε′ and μ′ at 2 GHz present the same trend as the content ratio (A(BCC)/A(FCC)), while the ε′′ improve obviously after annealing, corresponding to the elevation of conductivity. |
format | Online Article Text |
id | pubmed-9079992 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2018 |
publisher | The Royal Society of Chemistry |
record_format | MEDLINE/PubMed |
spelling | pubmed-90799922022-05-09 A new mechanism for improving electromagnetic properties based on tunable crystallographic structures of FeCoNiSi(x)Al(0.4) high entropy alloy powders Zhang, Bin Duan, Yuping Cui, Yulong Ma, Guojia Wang, Tongmin Dong, Xinglong RSC Adv Chemistry Mechanical grinding method was employed to prepare FeCoNiSi(x)Al(0.4) high entropy alloy powders, which present a simple solid solution structure (FCC and BCC). After annealing at 673 K, a large amount of BCC phase precipitate and a small amount of CoFe(2)O(4) phase generate. The change of crystal structure may lead to an increase in M(s) (from 100.3 emu g(−1) to 124.2 emu g(−1)) and a decrease in H(c) (from 107 Oe to 59.5 Oe for FeCoNiSi(0.3)Al(0.4)). The silica content has a significant effect on the electromagnetic parameters of the as-milled and as-annealed alloy powders, presenting the trend of first increase and then decrease. And the dielectric constant is obviously improved after annealing (e.g. from 8.48 to 11.21 and from 0.15 to 2.84 for the ε′ and ε′′ of FeCoNiSi(0.3)Al(0.4) at 18 GHz, respectively), while the permeability is reduced. Compared with those of the as-milled samples, the μ′ of as-annealed FeCoNiSi(x)Al(0.4) (x = 0.1, 0.3, 0.4) remain unchanged or even increase due to the formation of CoFe(2)O(4). Meanwhile, the relative content of the precipitated BCC to FCC for FeCoNiSi(0.3)Al(0.4) enhance with the annealing temperature increase from 573 K to 773 K, and then reduce. And the ε′ and μ′ at 2 GHz present the same trend as the content ratio (A(BCC)/A(FCC)), while the ε′′ improve obviously after annealing, corresponding to the elevation of conductivity. The Royal Society of Chemistry 2018-04-19 /pmc/articles/PMC9079992/ /pubmed/35541311 http://dx.doi.org/10.1039/c8ra01762j Text en This journal is © The Royal Society of Chemistry https://creativecommons.org/licenses/by-nc/3.0/ |
spellingShingle | Chemistry Zhang, Bin Duan, Yuping Cui, Yulong Ma, Guojia Wang, Tongmin Dong, Xinglong A new mechanism for improving electromagnetic properties based on tunable crystallographic structures of FeCoNiSi(x)Al(0.4) high entropy alloy powders |
title | A new mechanism for improving electromagnetic properties based on tunable crystallographic structures of FeCoNiSi(x)Al(0.4) high entropy alloy powders |
title_full | A new mechanism for improving electromagnetic properties based on tunable crystallographic structures of FeCoNiSi(x)Al(0.4) high entropy alloy powders |
title_fullStr | A new mechanism for improving electromagnetic properties based on tunable crystallographic structures of FeCoNiSi(x)Al(0.4) high entropy alloy powders |
title_full_unstemmed | A new mechanism for improving electromagnetic properties based on tunable crystallographic structures of FeCoNiSi(x)Al(0.4) high entropy alloy powders |
title_short | A new mechanism for improving electromagnetic properties based on tunable crystallographic structures of FeCoNiSi(x)Al(0.4) high entropy alloy powders |
title_sort | new mechanism for improving electromagnetic properties based on tunable crystallographic structures of feconisi(x)al(0.4) high entropy alloy powders |
topic | Chemistry |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9079992/ https://www.ncbi.nlm.nih.gov/pubmed/35541311 http://dx.doi.org/10.1039/c8ra01762j |
work_keys_str_mv | AT zhangbin anewmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT duanyuping anewmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT cuiyulong anewmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT maguojia anewmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT wangtongmin anewmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT dongxinglong anewmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT zhangbin newmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT duanyuping newmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT cuiyulong newmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT maguojia newmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT wangtongmin newmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders AT dongxinglong newmechanismforimprovingelectromagneticpropertiesbasedontunablecrystallographicstructuresoffeconisixal04highentropyalloypowders |