Cargando…

The influence of CePO(4) nanorods on the CO oxidation activity of Au/GdPO(4)-rods

In this work, Au/GdPO(4)-rods were found to be good catalysts for CO oxidation with a low content of Au. The dopant of CePO(4) could influence the activity of Au/GdPO(4) due to the synergistic effect. GdPO(4) and CePO(4) nanorods were obtained by a hydrothermal process and the Au/GdPO(4)-rod and Au/...

Descripción completa

Detalles Bibliográficos
Autores principales: Huanhuan, Yu, Fayun, Chen, Zhubaolin, Weiping, Huang, Shoumin, Zhang
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Royal Society of Chemistry 2018
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9080986/
https://www.ncbi.nlm.nih.gov/pubmed/35541729
http://dx.doi.org/10.1039/c8ra02206b
Descripción
Sumario:In this work, Au/GdPO(4)-rods were found to be good catalysts for CO oxidation with a low content of Au. The dopant of CePO(4) could influence the activity of Au/GdPO(4) due to the synergistic effect. GdPO(4) and CePO(4) nanorods were obtained by a hydrothermal process and the Au/GdPO(4)-rod and Au/Ce-GdPO(4)-rod catalysts were prepared by deposition–precipitation synthesis. The samples were extensively characterized by transmission electron microscopy (TEM), inductively coupled plasma (ICP), powder X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), ultraviolet-visible spectroscopy (UV-Vis), Fourier transform infrared spectroscopy (FT-IR), temperature programmed desorption (O(2)-TPD, CO-TPD, and CO(2)-TPD) and N(2) adsorption–desorption. The results showed that Au/GdPO(4) with a low Au content possessed good activity for CO oxidation. When the content of Ce is 25 at%, 0.5% Au/Ce-GdPO(4)-rods can convert CO completely at 65 °C, and the catalyst showed better high-temperature resistance than 0.5% Au/GdPO(4)-rods. 0.5% Au/Ce-GdPO(4)-rods also showed good stability at reaction temperatures of 55 and 65 °C with CO conversions of 90% and 100% after continuous operation for 12 h. They also showed no deactivation after 50 h at a relative high reaction temperature of 200 °C.