Study on mechanism of improving efficiency of permanent-magnet small ball-end magnetorheological polishing by increasing magnetorheological fluid temperature

Permanent-magnet small ball-end magnetorheological polishing method can be used to polish the small part with complex structure. However, the material removal rate of this method is low, which is difficult to improve the output and reduce the cost. In this research, the effect of magnetorheological...

Descripción completa

Detalles Bibliográficos
Autores principales: Tian, Jinchuan, Chen, Mingjun, Liu, Henan, Qin, Biao, Cheng, Jian, Sun, Yazhou
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Nature Publishing Group UK 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9095837/
https://www.ncbi.nlm.nih.gov/pubmed/35546348
http://dx.doi.org/10.1038/s41598-022-11937-8
Descripción
Sumario:Permanent-magnet small ball-end magnetorheological polishing method can be used to polish the small part with complex structure. However, the material removal rate of this method is low, which is difficult to improve the output and reduce the cost. In this research, the effect of magnetorheological fluid temperature on the material removal rate is theoretically analyzed by measuring the effect of temperature on the flow properties of magnetorheological fluid, establishing the hydrodynamic model of polishing zone and solving the material removal parameters. It is found that with the increase of the magnetorheological fluid temperature, the polishing relative velocity increases accordingly, which can promote the improvement of material removal rate. But the shear stress decreases accordingly, which inhibits the improvement of material removal rate. The verification experiment results show that the promoting effect can exceeds the inhibitory effect, so that the material removal rate increases with the increase of magnetorheological fluid temperature. When the magnetorheological fluid temperature increases to 60 °C, the material removal rate is improved by 108.4% and the polished surface roughness Sa can reach 14.9 nm. Therefore, increasing the magnetorheological fluid temperature can significantly improve the efficiency of permanent-magnet small ball-end magnetorheological polishing and obtain high quality polished surface.