High-Temperature Corrosion of Ni-Cr-Mo Cladding Layers with Different Si Contents in NaCl-KCl-Na(2)SO(4)-K(2)SO(4) Mixed Salt Medium
In this work, Ni-Cr-Mo cladding layers with different Si contents were prepared on Q235 steel using laser-cladding technology, and their corrosion characteristics were investigated in NaCl-KCl-Na(2)SO(4)-K(2)SO(4) mixed salt at 550 °C. The corrosion resistance of each cladding layer was tested by we...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9100067/ https://www.ncbi.nlm.nih.gov/pubmed/35591486 http://dx.doi.org/10.3390/ma15093152 |
Sumario: | In this work, Ni-Cr-Mo cladding layers with different Si contents were prepared on Q235 steel using laser-cladding technology, and their corrosion characteristics were investigated in NaCl-KCl-Na(2)SO(4)-K(2)SO(4) mixed salt at 550 °C. The corrosion resistance of each cladding layer was tested by weight loss method, and the phase compositions and microstructures of the cladding layers and corrosion products were determined by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results show that Si contributed to the formation of a dense chromium oxide film on the surface, and the addition of Si can significantly improve the corrosion resistance of the cladding layer at high temperature. At 550 °C, the corrosion rate of the cladding layer with 5 wt.% Si was only 38.2% of that of the cladding layer without Si. After 168 h of high-temperature corrosion, no Cr-rich oxide scale was found in the outermost layer of the Ni-Cr-Mo cladding layer without Si. When Si content was 3 wt.% and 5 wt.%, the Cr-rich oxide scale of the cladding layer was denser than that of the coating with 1 wt.% Si content. |
---|