High Densification of Tungsten via Hot Pressing at 1300 °C in Carbon Presence
A reactive sintering technique with a small addition of carbon (up to 1.9 wt.%) has been used for tungsten powder consolidation. The process allowed procurement of the nonporous and fully densified material at 1300 °C and 30 MPa in 12 min. The SEM and EDX analysis showed that the milling of 5 μm tun...
Autores principales: | Popov, Oleksii, Vishnyakov, Vladimir |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9144784/ https://www.ncbi.nlm.nih.gov/pubmed/35629665 http://dx.doi.org/10.3390/ma15103641 |
Ejemplares similares
-
Zirconium Carbide Produced by Spark Plasma Sintering and Hot Pressing: Densification Kinetics, Grain Growth, and Thermal Properties
por: Wei, Xialu, et al.
Publicado: (2016) -
Two-step hot isostatic pressing densification achieved non-porous fully-densified wood with enhanced physical and mechanical properties
por: Maturana, J. C., et al.
Publicado: (2023) -
Selective laser melting of high-performance pure tungsten: parameter design, densification behavior and mechanical properties
por: Tan, Chaolin, et al.
Publicado: (2018) -
Laser Powder Bed Fusion of Pure Tungsten: Effects of Process Parameters on Morphology, Densification, Microstructure
por: Li, Junfeng, et al.
Publicado: (2020) -
Effect of Hot Isostatic Pressing Process Parameters on Properties and Fracture Behavior of Tungsten Alloy Powders and Sintered Bars
por: Hu, Biao, et al.
Publicado: (2022)