Strengthening of 0.18 wt % C Steel by Cold Differential Speed Rolling
Steel sheets containing 0.18 wt % C were deformed by differential speed rolling (DSR) up to four passes and compared to the steel sheets processed by equal speed rolling (ESR). Not only microstructure, but also mechanical properties and rolling load, were studied, which enlightens the relationship b...
Autores principales: | Kang, Jee-Hyun, Ko, Young-Gun |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9144965/ https://www.ncbi.nlm.nih.gov/pubmed/35629742 http://dx.doi.org/10.3390/ma15103717 |
Ejemplares similares
-
Design of High Speed and Low Offset Dynamic Latch Comparator in 0.18 µm CMOS Process
por: Rahman, Labonnah Farzana, et al.
Publicado: (2014) -
Al(0.88)Cu(0.94)Fe(0.18)
por: Liu, Yibo, et al.
Publicado: (2023) -
Radiation Tolerant Design with 0.18-micron CMOS Technology
por: Chen, Li
Publicado: (2017) -
Precision Measurement of the $B_s-\kern0.18em\overline{\kern -0.18em B}{}^0_s$ Oscillation Frequency $\Delta m_s$ with $B_s\to D_s^-\pi^+$ Decays at LHCb
por: Heinicke, Kevin
Publicado: (2021) -
The Research of the Rolling Speed Influence on the Mechanism of Strip Breaks in the Steel Rolling Process
por: Rusnák, Ján, et al.
Publicado: (2020)