Repair of Bulk-Fill and Nanohybrid Resin Composites: Effect of Surface Conditioning, Adhesive Promoters, and Long-Term Aging

The aim of the study was to investigate the effect of different repair procedures on the repair bond strength of bulk-fill and nanohybrid resin composites after different aging periods. The resin composite blocks (8 × 8 × 4 mm(3)) were prepared from a bulk-fill (reliaFIL Bulk) and a nanohybrid (reli...

Descripción completa

Detalles Bibliográficos
Autores principales: Ugurlu, Muhittin, Al-Haj Husain, Nadin, Özcan, Mutlu
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9267362/
https://www.ncbi.nlm.nih.gov/pubmed/35806811
http://dx.doi.org/10.3390/ma15134688
_version_ 1784743700906115072
author Ugurlu, Muhittin
Al-Haj Husain, Nadin
Özcan, Mutlu
author_facet Ugurlu, Muhittin
Al-Haj Husain, Nadin
Özcan, Mutlu
author_sort Ugurlu, Muhittin
collection PubMed
description The aim of the study was to investigate the effect of different repair procedures on the repair bond strength of bulk-fill and nanohybrid resin composites after different aging periods. The resin composite blocks (8 × 8 × 4 mm(3)) were prepared from a bulk-fill (reliaFIL Bulk) and a nanohybrid (reliaFIL LC) resin composite and grouped according to aging duration (6 months, 1 year, and 2 years). Following aging, the blocks were assigned to different surface treatments; air-abrasion with aluminum oxide powder, roughening with a diamond bur, and no treatment. After cleansing with phosphoric acid, a silane layer (Porcelain Primer) was applied on the surface of half of the specimens in each group. The specimens were subdivided into two groups (n = 5): Scotchbond Universal (3M Oral Care) and All-Bond Universal (Bisco). The blocks were repaired with the nanohybrid composite (8 × 8 × 8 mm (3)). The repaired specimens were stored in distilled water (37 °C/24 h) and segmented into beams. Half of the beams were immediately subjected to microtensile μTBS testing (1 mm/min), while the other half was stored in distilled water (37 °C) for 6 months before testing. Failure modes were analyzed using stereomicroscope and SEM. Statistical analyses were performed with ANOVA and least significant difference tests (LSD) tests (p = 0.05). The extension of aging periods (6 months, 1 year, and 2 years) reduced the repair bond strength in some groups for both resin composites (p < 0.05). The air-abrasion and bur roughening improved the repair bond strength (p < 0.05). The silane application did not influence the repair bond strength and durability (p > 0.05). There was no difference among the universal adhesives in the same surface treatment groups (p > 0.05). The mechanical roughening treatments are necessary for the repair of resin composite. The universal adhesives might be used for the repair of resin composites regardless of silane content without prior silane application.
format Online
Article
Text
id pubmed-9267362
institution National Center for Biotechnology Information
language English
publishDate 2022
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-92673622022-07-09 Repair of Bulk-Fill and Nanohybrid Resin Composites: Effect of Surface Conditioning, Adhesive Promoters, and Long-Term Aging Ugurlu, Muhittin Al-Haj Husain, Nadin Özcan, Mutlu Materials (Basel) Article The aim of the study was to investigate the effect of different repair procedures on the repair bond strength of bulk-fill and nanohybrid resin composites after different aging periods. The resin composite blocks (8 × 8 × 4 mm(3)) were prepared from a bulk-fill (reliaFIL Bulk) and a nanohybrid (reliaFIL LC) resin composite and grouped according to aging duration (6 months, 1 year, and 2 years). Following aging, the blocks were assigned to different surface treatments; air-abrasion with aluminum oxide powder, roughening with a diamond bur, and no treatment. After cleansing with phosphoric acid, a silane layer (Porcelain Primer) was applied on the surface of half of the specimens in each group. The specimens were subdivided into two groups (n = 5): Scotchbond Universal (3M Oral Care) and All-Bond Universal (Bisco). The blocks were repaired with the nanohybrid composite (8 × 8 × 8 mm (3)). The repaired specimens were stored in distilled water (37 °C/24 h) and segmented into beams. Half of the beams were immediately subjected to microtensile μTBS testing (1 mm/min), while the other half was stored in distilled water (37 °C) for 6 months before testing. Failure modes were analyzed using stereomicroscope and SEM. Statistical analyses were performed with ANOVA and least significant difference tests (LSD) tests (p = 0.05). The extension of aging periods (6 months, 1 year, and 2 years) reduced the repair bond strength in some groups for both resin composites (p < 0.05). The air-abrasion and bur roughening improved the repair bond strength (p < 0.05). The silane application did not influence the repair bond strength and durability (p > 0.05). There was no difference among the universal adhesives in the same surface treatment groups (p > 0.05). The mechanical roughening treatments are necessary for the repair of resin composite. The universal adhesives might be used for the repair of resin composites regardless of silane content without prior silane application. MDPI 2022-07-04 /pmc/articles/PMC9267362/ /pubmed/35806811 http://dx.doi.org/10.3390/ma15134688 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Ugurlu, Muhittin
Al-Haj Husain, Nadin
Özcan, Mutlu
Repair of Bulk-Fill and Nanohybrid Resin Composites: Effect of Surface Conditioning, Adhesive Promoters, and Long-Term Aging
title Repair of Bulk-Fill and Nanohybrid Resin Composites: Effect of Surface Conditioning, Adhesive Promoters, and Long-Term Aging
title_full Repair of Bulk-Fill and Nanohybrid Resin Composites: Effect of Surface Conditioning, Adhesive Promoters, and Long-Term Aging
title_fullStr Repair of Bulk-Fill and Nanohybrid Resin Composites: Effect of Surface Conditioning, Adhesive Promoters, and Long-Term Aging
title_full_unstemmed Repair of Bulk-Fill and Nanohybrid Resin Composites: Effect of Surface Conditioning, Adhesive Promoters, and Long-Term Aging
title_short Repair of Bulk-Fill and Nanohybrid Resin Composites: Effect of Surface Conditioning, Adhesive Promoters, and Long-Term Aging
title_sort repair of bulk-fill and nanohybrid resin composites: effect of surface conditioning, adhesive promoters, and long-term aging
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9267362/
https://www.ncbi.nlm.nih.gov/pubmed/35806811
http://dx.doi.org/10.3390/ma15134688
work_keys_str_mv AT ugurlumuhittin repairofbulkfillandnanohybridresincompositeseffectofsurfaceconditioningadhesivepromotersandlongtermaging
AT alhajhusainnadin repairofbulkfillandnanohybridresincompositeseffectofsurfaceconditioningadhesivepromotersandlongtermaging
AT ozcanmutlu repairofbulkfillandnanohybridresincompositeseffectofsurfaceconditioningadhesivepromotersandlongtermaging