Size-Dependent Persistent Luminescence of YAGG:Cr(3+) Nanophosphors
In the current work, YAGG:Cr(3+) nanophosphors were synthesized by the Pechini method and then annealed at different temperatures in the range 800–1300 °C. The structure and morphology of the samples were characterized by X-ray Powder Diffraction (XRPD). The lattice parameters and average crystallin...
Autores principales: | Boiko, Vitalii, Dai, Zhengfa, Chaika, Mykhailo, Grzeszkiewicz, Karina, Li, Jiang, Strek, Wieslaw, Hreniak, Dariusz |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9267483/ https://www.ncbi.nlm.nih.gov/pubmed/35806532 http://dx.doi.org/10.3390/ma15134407 |
Ejemplares similares
-
Urea Glass
Route as a Way to Optimize YAGG:Ce(3+),Cr(3+),Pr(3+) Nanocrystals for Persistent
Luminescence Applications
por: Boiko, Vitalii, et al.
Publicado: (2022) -
Particle size-related limitations of persistent phosphors based on the doped Y(3)Al(2)Ga(3)O(12) system
por: Boiko, Vitalii, et al.
Publicado: (2021) -
Lanthanide-Doped Luminescent Nanophosphors via Ionic Liquids
por: Sharma, Rahul Kumar, et al.
Publicado: (2021) -
Engineering of bulk and fiber-shaped YAGG:Ce scintillator crystals
por: Sidletskiy, O, et al.
Publicado: (2017) -
Luminescence properties of ZnGa(2)O(4):Cr(3+),Bi(3+) nanophosphors for thermometry applications
por: Glais, E., et al.
Publicado: (2018)