Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario
The present study aimed to evaluate the wear rate of polymer-infiltrated network composites and ceramics against enamel in a bruxism-simulated scenario. Ninety-six (n = 96) molars were divided into six groups (n = 16) according to their occlusal material: group 1—a polymer-infiltrated network cerami...
Autores principales: | , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9313215/ https://www.ncbi.nlm.nih.gov/pubmed/35884986 http://dx.doi.org/10.3390/biomedicines10071682 |
_version_ | 1784754024907538432 |
---|---|
author | Baldi, Andrea Carossa, Massimo Comba, Allegra Alovisi, Mario Femiano, Felice Pasqualini, Damiano Berutti, Elio Scotti, Nicola |
author_facet | Baldi, Andrea Carossa, Massimo Comba, Allegra Alovisi, Mario Femiano, Felice Pasqualini, Damiano Berutti, Elio Scotti, Nicola |
author_sort | Baldi, Andrea |
collection | PubMed |
description | The present study aimed to evaluate the wear rate of polymer-infiltrated network composites and ceramics against enamel in a bruxism-simulated scenario. Ninety-six (n = 96) molars were divided into six groups (n = 16) according to their occlusal material: group 1—a polymer-infiltrated network ceramic (PINC); group 2—a second polymer-infiltrated network ceramic (PINC2); group 3—nanohybrid resin-based composite (CO); group 4—cubic zirconia (ZR); group 5—lithium disilicate (LS); and group 6—sound enamel (EN). A laser scanner was used to digitalize all of the occlusal surfaces before and after a fatigue test, which was conducted with a chewing simulator set at 80 N and semicircular movement in order to simulate bruxist movement and loads. Statistical analysis of volume loss was performed with a one-way ANOVA and post hoc Bonferroni test. ZR had significantly inferior wear to PINC (p ≤ 0.01) and CO (p = 0.04). LS wore the antagonist enamel significantly more than PINC, CO, PINC2 and EN (p ≤ 0.01). On the other hand, ZR wore the antagonist enamel significantly more than CO (p ≤ 0.01) and PINC2 (p = 0.05). In conclusion, PINCs better preserved antagonist enamel at the expense of a higher wear of their own. LS causes significantly higher enamel wear compared with PINCs. ZR caused significantly higher enamel wear compared with CO and PINC2, but it was wear-resistant. |
format | Online Article Text |
id | pubmed-9313215 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2022 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-93132152022-07-26 Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario Baldi, Andrea Carossa, Massimo Comba, Allegra Alovisi, Mario Femiano, Felice Pasqualini, Damiano Berutti, Elio Scotti, Nicola Biomedicines Article The present study aimed to evaluate the wear rate of polymer-infiltrated network composites and ceramics against enamel in a bruxism-simulated scenario. Ninety-six (n = 96) molars were divided into six groups (n = 16) according to their occlusal material: group 1—a polymer-infiltrated network ceramic (PINC); group 2—a second polymer-infiltrated network ceramic (PINC2); group 3—nanohybrid resin-based composite (CO); group 4—cubic zirconia (ZR); group 5—lithium disilicate (LS); and group 6—sound enamel (EN). A laser scanner was used to digitalize all of the occlusal surfaces before and after a fatigue test, which was conducted with a chewing simulator set at 80 N and semicircular movement in order to simulate bruxist movement and loads. Statistical analysis of volume loss was performed with a one-way ANOVA and post hoc Bonferroni test. ZR had significantly inferior wear to PINC (p ≤ 0.01) and CO (p = 0.04). LS wore the antagonist enamel significantly more than PINC, CO, PINC2 and EN (p ≤ 0.01). On the other hand, ZR wore the antagonist enamel significantly more than CO (p ≤ 0.01) and PINC2 (p = 0.05). In conclusion, PINCs better preserved antagonist enamel at the expense of a higher wear of their own. LS causes significantly higher enamel wear compared with PINCs. ZR caused significantly higher enamel wear compared with CO and PINC2, but it was wear-resistant. MDPI 2022-07-12 /pmc/articles/PMC9313215/ /pubmed/35884986 http://dx.doi.org/10.3390/biomedicines10071682 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Baldi, Andrea Carossa, Massimo Comba, Allegra Alovisi, Mario Femiano, Felice Pasqualini, Damiano Berutti, Elio Scotti, Nicola Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario |
title | Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario |
title_full | Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario |
title_fullStr | Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario |
title_full_unstemmed | Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario |
title_short | Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario |
title_sort | wear behaviour of polymer-infiltrated network ceramics, lithium disilicate and cubic zirconia against enamel in a bruxism-simulated scenario |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9313215/ https://www.ncbi.nlm.nih.gov/pubmed/35884986 http://dx.doi.org/10.3390/biomedicines10071682 |
work_keys_str_mv | AT baldiandrea wearbehaviourofpolymerinfiltratednetworkceramicslithiumdisilicateandcubiczirconiaagainstenamelinabruxismsimulatedscenario AT carossamassimo wearbehaviourofpolymerinfiltratednetworkceramicslithiumdisilicateandcubiczirconiaagainstenamelinabruxismsimulatedscenario AT combaallegra wearbehaviourofpolymerinfiltratednetworkceramicslithiumdisilicateandcubiczirconiaagainstenamelinabruxismsimulatedscenario AT alovisimario wearbehaviourofpolymerinfiltratednetworkceramicslithiumdisilicateandcubiczirconiaagainstenamelinabruxismsimulatedscenario AT femianofelice wearbehaviourofpolymerinfiltratednetworkceramicslithiumdisilicateandcubiczirconiaagainstenamelinabruxismsimulatedscenario AT pasqualinidamiano wearbehaviourofpolymerinfiltratednetworkceramicslithiumdisilicateandcubiczirconiaagainstenamelinabruxismsimulatedscenario AT beruttielio wearbehaviourofpolymerinfiltratednetworkceramicslithiumdisilicateandcubiczirconiaagainstenamelinabruxismsimulatedscenario AT scottinicola wearbehaviourofpolymerinfiltratednetworkceramicslithiumdisilicateandcubiczirconiaagainstenamelinabruxismsimulatedscenario |