Stability Study of the Irradiated Poly(lactic acid)/Styrene Isoprene Styrene Reinforced with Silica Nanoparticles

In this paper, the stability improvement of poly(lactic acid) (PLA)/styrene-isoprene block copolymer (SIS) loaded with silica nanoparticles is characterized. The protection efficiency in the material of thermal stability is mainly studied by means of high accurate isothermal and nonisothermal chemil...

Descripción completa

Detalles Bibliográficos
Autores principales: Lupu (Luchian), Ana Maria, Mariş, Marius, Zaharescu, Traian, Marinescu, Virgil Emanuel, Iovu, Horia
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9319368/
https://www.ncbi.nlm.nih.gov/pubmed/35888545
http://dx.doi.org/10.3390/ma15145080
_version_ 1784755532124389376
author Lupu (Luchian), Ana Maria
Mariş, Marius
Zaharescu, Traian
Marinescu, Virgil Emanuel
Iovu, Horia
author_facet Lupu (Luchian), Ana Maria
Mariş, Marius
Zaharescu, Traian
Marinescu, Virgil Emanuel
Iovu, Horia
author_sort Lupu (Luchian), Ana Maria
collection PubMed
description In this paper, the stability improvement of poly(lactic acid) (PLA)/styrene-isoprene block copolymer (SIS) loaded with silica nanoparticles is characterized. The protection efficiency in the material of thermal stability is mainly studied by means of high accurate isothermal and nonisothermal chemiluminescence procedures. The oxidation induction times obtained in the isothermal CL determinations increase from 45 min to 312 min as the polymer is free of silica or the filler loading is about 10%, respectively. The nonisothermal measurements reveal the values of onset oxidation temperatures with about 15% when the concentration of SiO(2) particles is enhanced from none to 10%. The curing assay and Charlesby–Pinner representation as well as the modifications that occurred in the FTIR carbonyl band at 1745 cm(−1) are appropriate proofs for the delay of oxidation in hybrid samples. The improved efficiency of silica during the accelerated degradation of PLA/SIS 30/n-SiO(2) composites is demonstrated by means of the increased values of activation energy in correlation with the augmentation of silica loading. While the pristine material is modified by the addition of 10% silica nanoparticles, the activation energy grows from 55 kJ mol(−1) to 74 kJ mol(−1) for nonirradiated samples and from 47 kJ mol(−1) to 76 kJ mol(−1) for γ-processed material at 25 kGy. The stabilizer features are associated with silica nanoparticles due to the protection of fragments generated by the scission of hydrocarbon structure of SIS, the minor component, whose degradation fragments are early converted into hydroperoxides rather than influencing depolymerization in the PLA phase. The reduction of the transmission values concerning the growing reinforcement is evidence of the capacity of SiO(2) to minimize the changes in polymers subjected to high energy sterilization. The silica loading of 10 wt% may be considered a proper solution for attaining an extended lifespan under the accelerated degradation caused by the intense transfer of energy, such as radiation processing on the polymer hybrid.
format Online
Article
Text
id pubmed-9319368
institution National Center for Biotechnology Information
language English
publishDate 2022
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-93193682022-07-27 Stability Study of the Irradiated Poly(lactic acid)/Styrene Isoprene Styrene Reinforced with Silica Nanoparticles Lupu (Luchian), Ana Maria Mariş, Marius Zaharescu, Traian Marinescu, Virgil Emanuel Iovu, Horia Materials (Basel) Article In this paper, the stability improvement of poly(lactic acid) (PLA)/styrene-isoprene block copolymer (SIS) loaded with silica nanoparticles is characterized. The protection efficiency in the material of thermal stability is mainly studied by means of high accurate isothermal and nonisothermal chemiluminescence procedures. The oxidation induction times obtained in the isothermal CL determinations increase from 45 min to 312 min as the polymer is free of silica or the filler loading is about 10%, respectively. The nonisothermal measurements reveal the values of onset oxidation temperatures with about 15% when the concentration of SiO(2) particles is enhanced from none to 10%. The curing assay and Charlesby–Pinner representation as well as the modifications that occurred in the FTIR carbonyl band at 1745 cm(−1) are appropriate proofs for the delay of oxidation in hybrid samples. The improved efficiency of silica during the accelerated degradation of PLA/SIS 30/n-SiO(2) composites is demonstrated by means of the increased values of activation energy in correlation with the augmentation of silica loading. While the pristine material is modified by the addition of 10% silica nanoparticles, the activation energy grows from 55 kJ mol(−1) to 74 kJ mol(−1) for nonirradiated samples and from 47 kJ mol(−1) to 76 kJ mol(−1) for γ-processed material at 25 kGy. The stabilizer features are associated with silica nanoparticles due to the protection of fragments generated by the scission of hydrocarbon structure of SIS, the minor component, whose degradation fragments are early converted into hydroperoxides rather than influencing depolymerization in the PLA phase. The reduction of the transmission values concerning the growing reinforcement is evidence of the capacity of SiO(2) to minimize the changes in polymers subjected to high energy sterilization. The silica loading of 10 wt% may be considered a proper solution for attaining an extended lifespan under the accelerated degradation caused by the intense transfer of energy, such as radiation processing on the polymer hybrid. MDPI 2022-07-21 /pmc/articles/PMC9319368/ /pubmed/35888545 http://dx.doi.org/10.3390/ma15145080 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Lupu (Luchian), Ana Maria
Mariş, Marius
Zaharescu, Traian
Marinescu, Virgil Emanuel
Iovu, Horia
Stability Study of the Irradiated Poly(lactic acid)/Styrene Isoprene Styrene Reinforced with Silica Nanoparticles
title Stability Study of the Irradiated Poly(lactic acid)/Styrene Isoprene Styrene Reinforced with Silica Nanoparticles
title_full Stability Study of the Irradiated Poly(lactic acid)/Styrene Isoprene Styrene Reinforced with Silica Nanoparticles
title_fullStr Stability Study of the Irradiated Poly(lactic acid)/Styrene Isoprene Styrene Reinforced with Silica Nanoparticles
title_full_unstemmed Stability Study of the Irradiated Poly(lactic acid)/Styrene Isoprene Styrene Reinforced with Silica Nanoparticles
title_short Stability Study of the Irradiated Poly(lactic acid)/Styrene Isoprene Styrene Reinforced with Silica Nanoparticles
title_sort stability study of the irradiated poly(lactic acid)/styrene isoprene styrene reinforced with silica nanoparticles
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9319368/
https://www.ncbi.nlm.nih.gov/pubmed/35888545
http://dx.doi.org/10.3390/ma15145080
work_keys_str_mv AT lupuluchiananamaria stabilitystudyoftheirradiatedpolylacticacidstyreneisoprenestyrenereinforcedwithsilicananoparticles
AT marismarius stabilitystudyoftheirradiatedpolylacticacidstyreneisoprenestyrenereinforcedwithsilicananoparticles
AT zaharescutraian stabilitystudyoftheirradiatedpolylacticacidstyreneisoprenestyrenereinforcedwithsilicananoparticles
AT marinescuvirgilemanuel stabilitystudyoftheirradiatedpolylacticacidstyreneisoprenestyrenereinforcedwithsilicananoparticles
AT iovuhoria stabilitystudyoftheirradiatedpolylacticacidstyreneisoprenestyrenereinforcedwithsilicananoparticles