Cargando…

Polymethylmethacrylate Incorporating Nanodiamonds for Denture Repair: In Vitro Study on the Mechanical Properties

Objective  This study aimed to evaluate the effect of nanodiamond (ND) addition to repair resin with repair gap modifications on the flexural and impact strength of repaired polymethylmethacrylate denture base. Materials and Methods  Heat-polymerized acrylic resin specimens ( N  = 100/test) were pre...

Descripción completa

Detalles Bibliográficos
Autores principales: Gad, Mohammed M., Ali, Mohamed Saber, Al-Thobity, Ahmad M., Al-Dulaijan, Yousif A., Zayat, Mai El, Emam, Abdel-Naser M., Akhtar, Sultan, Khan, Soban Q., Al-Harbi, Fahad A., Fouda, Shaimaa M.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Thieme Medical and Scientific Publishers Pvt. Ltd. 2021
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9339932/
https://www.ncbi.nlm.nih.gov/pubmed/34823262
http://dx.doi.org/10.1055/s-0041-1735792
_version_ 1784760282986315776
author Gad, Mohammed M.
Ali, Mohamed Saber
Al-Thobity, Ahmad M.
Al-Dulaijan, Yousif A.
Zayat, Mai El
Emam, Abdel-Naser M.
Akhtar, Sultan
Khan, Soban Q.
Al-Harbi, Fahad A.
Fouda, Shaimaa M.
author_facet Gad, Mohammed M.
Ali, Mohamed Saber
Al-Thobity, Ahmad M.
Al-Dulaijan, Yousif A.
Zayat, Mai El
Emam, Abdel-Naser M.
Akhtar, Sultan
Khan, Soban Q.
Al-Harbi, Fahad A.
Fouda, Shaimaa M.
author_sort Gad, Mohammed M.
collection PubMed
description Objective  This study aimed to evaluate the effect of nanodiamond (ND) addition to repair resin with repair gap modifications on the flexural and impact strength of repaired polymethylmethacrylate denture base. Materials and Methods  Heat-polymerized acrylic resin specimens ( N  = 100/test) were prepared and sectioned to half creating two repair gaps: 2.5- and 0 mm with 45 degrees beveling. They were further divided into subgroups ( n  = 20) according to ND concentration (control, 0.25%ND, and 0.50%ND), thermocycling (500 cycles) was done to half the specimens in each subgroup. Flexural strength was tested using 3-point bending test and impact strength was tested by Charpy's impact test. Analysis of variance and post-hoc Tukey's tests were performed for data analysis ( α  = 0.05). Scanning electron microscope was employed for fracture surface analysis and ND distribution. Results  Before and after thermocycling, the addition of ND significantly increased the flexural strength and elastic modulus in comparison to control group ( p ˂ 0.001), while 0 mm repair gap showed insignificant difference between ND-reinforced groups ( p ˃ 0.05). Regarding impact strength, ND addition increased the impact strength with 0 mm gap in comparison to control and 2.5 mm with ND ( p ˂0.001), while later groups showed no significant in between ( p ˃ 0.05). Comparing thermocycling effect per respective concentration and repair gap, thermocycling adversely affected all tested properties except elastic modulus with 0 mm–0.25 and 0 mm–0.5% and impact strength with 2.5 mm, 2.5 mm–0.25%, 2.5 mm– 0.5% ( p ˃ 0.05). Conclusion  ND addition combined with decreased repair gap improved the flexural strength, elastic modulus, and impact strength of repaired denture resin, while thermocycling has a negative effect on denture repair strength.
format Online
Article
Text
id pubmed-9339932
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher Thieme Medical and Scientific Publishers Pvt. Ltd.
record_format MEDLINE/PubMed
spelling pubmed-93399322022-08-02 Polymethylmethacrylate Incorporating Nanodiamonds for Denture Repair: In Vitro Study on the Mechanical Properties Gad, Mohammed M. Ali, Mohamed Saber Al-Thobity, Ahmad M. Al-Dulaijan, Yousif A. Zayat, Mai El Emam, Abdel-Naser M. Akhtar, Sultan Khan, Soban Q. Al-Harbi, Fahad A. Fouda, Shaimaa M. Eur J Dent Objective  This study aimed to evaluate the effect of nanodiamond (ND) addition to repair resin with repair gap modifications on the flexural and impact strength of repaired polymethylmethacrylate denture base. Materials and Methods  Heat-polymerized acrylic resin specimens ( N  = 100/test) were prepared and sectioned to half creating two repair gaps: 2.5- and 0 mm with 45 degrees beveling. They were further divided into subgroups ( n  = 20) according to ND concentration (control, 0.25%ND, and 0.50%ND), thermocycling (500 cycles) was done to half the specimens in each subgroup. Flexural strength was tested using 3-point bending test and impact strength was tested by Charpy's impact test. Analysis of variance and post-hoc Tukey's tests were performed for data analysis ( α  = 0.05). Scanning electron microscope was employed for fracture surface analysis and ND distribution. Results  Before and after thermocycling, the addition of ND significantly increased the flexural strength and elastic modulus in comparison to control group ( p ˂ 0.001), while 0 mm repair gap showed insignificant difference between ND-reinforced groups ( p ˃ 0.05). Regarding impact strength, ND addition increased the impact strength with 0 mm gap in comparison to control and 2.5 mm with ND ( p ˂0.001), while later groups showed no significant in between ( p ˃ 0.05). Comparing thermocycling effect per respective concentration and repair gap, thermocycling adversely affected all tested properties except elastic modulus with 0 mm–0.25 and 0 mm–0.5% and impact strength with 2.5 mm, 2.5 mm–0.25%, 2.5 mm– 0.5% ( p ˃ 0.05). Conclusion  ND addition combined with decreased repair gap improved the flexural strength, elastic modulus, and impact strength of repaired denture resin, while thermocycling has a negative effect on denture repair strength. Thieme Medical and Scientific Publishers Pvt. Ltd. 2021-11-25 /pmc/articles/PMC9339932/ /pubmed/34823262 http://dx.doi.org/10.1055/s-0041-1735792 Text en The Author(s). This is an open access article published by Thieme under the terms of the Creative Commons Attribution License, permitting unrestricted use, distribution, and reproduction so long as the original work is properly cited. ( https://creativecommons.org/licenses/by/4.0/ ) https://creativecommons.org/licenses/by/4.0/This is an open-access article distributed under the terms of the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
spellingShingle Gad, Mohammed M.
Ali, Mohamed Saber
Al-Thobity, Ahmad M.
Al-Dulaijan, Yousif A.
Zayat, Mai El
Emam, Abdel-Naser M.
Akhtar, Sultan
Khan, Soban Q.
Al-Harbi, Fahad A.
Fouda, Shaimaa M.
Polymethylmethacrylate Incorporating Nanodiamonds for Denture Repair: In Vitro Study on the Mechanical Properties
title Polymethylmethacrylate Incorporating Nanodiamonds for Denture Repair: In Vitro Study on the Mechanical Properties
title_full Polymethylmethacrylate Incorporating Nanodiamonds for Denture Repair: In Vitro Study on the Mechanical Properties
title_fullStr Polymethylmethacrylate Incorporating Nanodiamonds for Denture Repair: In Vitro Study on the Mechanical Properties
title_full_unstemmed Polymethylmethacrylate Incorporating Nanodiamonds for Denture Repair: In Vitro Study on the Mechanical Properties
title_short Polymethylmethacrylate Incorporating Nanodiamonds for Denture Repair: In Vitro Study on the Mechanical Properties
title_sort polymethylmethacrylate incorporating nanodiamonds for denture repair: in vitro study on the mechanical properties
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9339932/
https://www.ncbi.nlm.nih.gov/pubmed/34823262
http://dx.doi.org/10.1055/s-0041-1735792
work_keys_str_mv AT gadmohammedm polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties
AT alimohamedsaber polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties
AT althobityahmadm polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties
AT aldulaijanyousifa polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties
AT zayatmaiel polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties
AT emamabdelnaserm polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties
AT akhtarsultan polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties
AT khansobanq polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties
AT alharbifahada polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties
AT foudashaimaam polymethylmethacrylateincorporatingnanodiamondsfordenturerepairinvitrostudyonthemechanicalproperties