Evaluation of a Method to Determine Wear Resistance of Class I Tooth Restorations during Cyclic Loading

The aim of this study was the development of a test regime to determine the wear resistance and predict the clinical performance of conventional glass ionomer cement (GIC) restorations in Class I tooth cavities. Cavities were prepared in excised human teeth and restored using three conventional glas...

Descripción completa

Detalles Bibliográficos
Autores principales: Messer-Hannemann, Philipp, Samadi, Mariam, Böttcher, Henrik, Duy, Sebastian, Duy, Daniela, Albrecht, Niclas, Schwendicke, Falk, Effenberger, Susanne
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9369466/
https://www.ncbi.nlm.nih.gov/pubmed/35955375
http://dx.doi.org/10.3390/ma15155440
Descripción
Sumario:The aim of this study was the development of a test regime to determine the wear resistance and predict the clinical performance of conventional glass ionomer cement (GIC) restorations in Class I tooth cavities. Cavities were prepared in excised human teeth and restored using three conventional glass ionomer restorative materials: DeltaFil, Fuji IX GP and Ketac Universal. The restored teeth were mechanically and thermally stressed using a chewing simulator with a maximum number of 1,200,000 load cycles. Besides determining the number of cycles achieved, the abrasion volume after termination of the chewing simulation was calculated using µCT images. All teeth restored with DeltaFil reached 1,200,000 cycles without any restoration failure. Only 37.5% of the restorations each with Ketac Universal and Fuji IX GP were able to achieve the maximum cycle number. A significant lower abrasion volume for restorations with DeltaFil compared to Ketac Universal (p = 0.0099) and Fuji IX GP (p = 0.0005) was found. Laboratory chewing simulations are a useful tool to study basic wear mechanisms in a controlled setting with in-vivo related parameters. DeltaFil shows an improved wear resistance compared to other conventional GICs, indicating the high potential of this material for long-lasting Class I restorations.