Colour Stability of 3D-Printed and Prefabricated Denture Teeth after Immersion in Different Colouring Agents—An In Vitro Study

This study investigated the colour stability of three dimensional (3D)-printed and conventional denture teeth after immersion in different colourants. A total of 60 artificial maxillary central incisors were selected from three types of materials: 3D-printed dental resin (NextDent, 3D Systems, Soest...

Descripción completa

Detalles Bibliográficos
Autores principales: Dimitrova, Mariya, Chuchulska, Bozhana, Zlatev, Stefan, Kazakova, Rada
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9371044/
https://www.ncbi.nlm.nih.gov/pubmed/35956640
http://dx.doi.org/10.3390/polym14153125
Descripción
Sumario:This study investigated the colour stability of three dimensional (3D)-printed and conventional denture teeth after immersion in different colourants. A total of 60 artificial maxillary central incisors were selected from three types of materials: 3D-printed dental resin (NextDent, 3D Systems, Soesterberg, The Netherlands), prefabricated acrylic teeth in Ivostar Shade (Ivoclar Vivadent, Schaan, Liechtenstein), and SpofaDent Plus in shade A2 (SpofaDental, Jičín, Czechia). These were immersed in four types of colourants at room temperature (23 °C ± 1 °C), including artificial saliva (pH = 6.8) as a control group, coffee, red wine, and Coca-Cola (n = 5). The temperature and the pH of the colouring agents were maintained throughout all immersion periods. After 7 days (T1), 14 days (T2), and 21 days (T3), the ∆E values were measured with a SpectroShade Micro (SpectroShade, Oxnard, CA, USA) spectrophotometer. Their means were then calculated and compared by two-way ANOVA. The independent factors, immersion time and different staining solutions, as well as the interaction between these factors, significantly influenced ΔE. The highest and the lowest mean ∆Es were recorded for prefabricated teeth in red wine, and 3D-printed teeth in artificial saliva, respectively. All the specimens demonstrated an increased colour change at T1 compared to T3, and the difference in mean ∆E was statistically significant.