Microstructure Evolution and Mechanical Properties of 20%SiC(p)/Al Joint Prepared via Laser Welding

SiC particles-reinforced Al matrix composites (SiC(p)/AMCs) have been widely used in the aerospace structural components. In this work, 20 vol% SiC(p)/2A14 joint was fabricated by laser welding technology. The effects of different laser power/welding velocity on the 20 vol% SiC(p)/2A14 joint forming...