Effect of Curing Temperature on the Properties of a MgO-SiO(2)-H(2)O System Prepared Using Dead-Burned MgO

The hydration of M-S-H prepared using silica fume (SF) and dead-burned MgO cured at 20 °C, 50 °C, and 80 °C was investigated, and the properties and performance of this M-S-H were measured. The formation of M-S-H was characterized using XRD, FTIR, TGA, and (29)Si MAS-NMR. Results show that the compr...

Descripción completa

Detalles Bibliográficos
Autores principales: Cheng, Fuan, Hu, Yaru, Song, Qiang, Nie, Jiao, Su, Jiahao, Chen, Yanxin
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9457786/
https://www.ncbi.nlm.nih.gov/pubmed/36079446
http://dx.doi.org/10.3390/ma15176065
Descripción
Sumario:The hydration of M-S-H prepared using silica fume (SF) and dead-burned MgO cured at 20 °C, 50 °C, and 80 °C was investigated, and the properties and performance of this M-S-H were measured. The formation of M-S-H was characterized using XRD, FTIR, TGA, and (29)Si MAS-NMR. Results show that the compressive strength of paste prepared using MgO calcined at 1450 °C for 2 h reached 25 MPa after 28 d. The shrinkage of mortar made with low reactivity MgO was lower than that made with high reactivity MgO. The pH value of MgO/SF paste mixed with dead-burned MgO did not exceed 10.4 at room temperature. The shrinkage of M-S-H prepared using dead-burned MgO was less than that prepared using more active MgO, and its strength did not decrease over time. No (or only a small amount of) Mg(OH)(2) was formed, which is why the strength of M-S-H prepared with dead-burned MgO continually increased, without decreasing. The promotion of curing temperature favor process of MgO hydration and is beneficial for degree of silica polymerization. The sample cured in 50 °C water showed the highest relative degree of reaction.