Cargando…
Ultrafine-Grained Tungsten Heavy Alloy Prepared by High-Pressure Spark Plasma Sintering
Tungsten heavy alloy (WHA) is an ideal material employed for kinetic energy penetrators due to its high density and excellent mechanical properties. However, it is difficult to obtain ultrafine-grained tungsten alloy with excellent properties by traditional powder metallurgy method because of severe...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9457849/ https://www.ncbi.nlm.nih.gov/pubmed/36079552 http://dx.doi.org/10.3390/ma15176168 |
_version_ | 1784786157237698560 |
---|---|
author | Zhang, Shuaihao Zhu, Qiqi Li, Qiunan Ji, Wei Wang, Weimin Fu, Zhengyi |
author_facet | Zhang, Shuaihao Zhu, Qiqi Li, Qiunan Ji, Wei Wang, Weimin Fu, Zhengyi |
author_sort | Zhang, Shuaihao |
collection | PubMed |
description | Tungsten heavy alloy (WHA) is an ideal material employed for kinetic energy penetrators due to its high density and excellent mechanical properties. However, it is difficult to obtain ultrafine-grained tungsten alloy with excellent properties by traditional powder metallurgy method because of severe grain growth at a high sintering temperature with a long soaking time. In this study, the sintering behavior of tungsten alloys was studied at 800 to 1300 °C, and highly dense 93W-5.6Ni-1.4Fe (wt.%) WHA was successfully fabricated at a low temperature of 950 °C with a high pressure of 150 MPa by spark plasma sintering. The as-sintered tungsten alloy possesses a high relative density (98.6%), ultrafine grain size (271 nm) and high dislocation density (2.6 × 10(16) m(−2)), which results in excellent properties such as a high hardness (1079 HV1). The high sintering pressure is considered to support an additional driving force for the sintering and lead to a low-temperature densification, which effectively limits grain growth. |
format | Online Article Text |
id | pubmed-9457849 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2022 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-94578492022-09-09 Ultrafine-Grained Tungsten Heavy Alloy Prepared by High-Pressure Spark Plasma Sintering Zhang, Shuaihao Zhu, Qiqi Li, Qiunan Ji, Wei Wang, Weimin Fu, Zhengyi Materials (Basel) Article Tungsten heavy alloy (WHA) is an ideal material employed for kinetic energy penetrators due to its high density and excellent mechanical properties. However, it is difficult to obtain ultrafine-grained tungsten alloy with excellent properties by traditional powder metallurgy method because of severe grain growth at a high sintering temperature with a long soaking time. In this study, the sintering behavior of tungsten alloys was studied at 800 to 1300 °C, and highly dense 93W-5.6Ni-1.4Fe (wt.%) WHA was successfully fabricated at a low temperature of 950 °C with a high pressure of 150 MPa by spark plasma sintering. The as-sintered tungsten alloy possesses a high relative density (98.6%), ultrafine grain size (271 nm) and high dislocation density (2.6 × 10(16) m(−2)), which results in excellent properties such as a high hardness (1079 HV1). The high sintering pressure is considered to support an additional driving force for the sintering and lead to a low-temperature densification, which effectively limits grain growth. MDPI 2022-09-05 /pmc/articles/PMC9457849/ /pubmed/36079552 http://dx.doi.org/10.3390/ma15176168 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Zhang, Shuaihao Zhu, Qiqi Li, Qiunan Ji, Wei Wang, Weimin Fu, Zhengyi Ultrafine-Grained Tungsten Heavy Alloy Prepared by High-Pressure Spark Plasma Sintering |
title | Ultrafine-Grained Tungsten Heavy Alloy Prepared by High-Pressure Spark Plasma Sintering |
title_full | Ultrafine-Grained Tungsten Heavy Alloy Prepared by High-Pressure Spark Plasma Sintering |
title_fullStr | Ultrafine-Grained Tungsten Heavy Alloy Prepared by High-Pressure Spark Plasma Sintering |
title_full_unstemmed | Ultrafine-Grained Tungsten Heavy Alloy Prepared by High-Pressure Spark Plasma Sintering |
title_short | Ultrafine-Grained Tungsten Heavy Alloy Prepared by High-Pressure Spark Plasma Sintering |
title_sort | ultrafine-grained tungsten heavy alloy prepared by high-pressure spark plasma sintering |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9457849/ https://www.ncbi.nlm.nih.gov/pubmed/36079552 http://dx.doi.org/10.3390/ma15176168 |
work_keys_str_mv | AT zhangshuaihao ultrafinegrainedtungstenheavyalloypreparedbyhighpressuresparkplasmasintering AT zhuqiqi ultrafinegrainedtungstenheavyalloypreparedbyhighpressuresparkplasmasintering AT liqiunan ultrafinegrainedtungstenheavyalloypreparedbyhighpressuresparkplasmasintering AT jiwei ultrafinegrainedtungstenheavyalloypreparedbyhighpressuresparkplasmasintering AT wangweimin ultrafinegrainedtungstenheavyalloypreparedbyhighpressuresparkplasmasintering AT fuzhengyi ultrafinegrainedtungstenheavyalloypreparedbyhighpressuresparkplasmasintering |