Effect of Impact Velocity and Angle on Impact Wear Behavior of Zr-4 Alloy Cladding Tube

In the pressurized water reactor nuclear power plant, 316L SS chips were captured by the support grid and continued to affect the Zr-4 cladding tube, causing the fuel rods to wear and perforate. In this work, a 60° acute angle cone of 316L SS was used to simulate the cyclic impact of debris on a Zr-...

Descripción completa

Detalles Bibliográficos
Autores principales: Yu, Shi-Jia, Hu, Yong, Liu, Xin, Li, Dong-Xing, He, Li-Ping, Wang, Jun, Cai, Zhen-Bing
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9505043/
https://www.ncbi.nlm.nih.gov/pubmed/36143684
http://dx.doi.org/10.3390/ma15186371
Descripción
Sumario:In the pressurized water reactor nuclear power plant, 316L SS chips were captured by the support grid and continued to affect the Zr-4 cladding tube, causing the fuel rods to wear and perforate. In this work, a 60° acute angle cone of 316L SS was used to simulate the cyclic impact of debris on a Zr-4 alloy tube with different initial impact velocities and impact angles. Results showed that increasing the initial impact velocity will generate a wear debris accumulation layer with a wear-reducing effect, but also promote the extension and expansion of fatigue cracks, resulting in the delamination of Zr-4 alloy tubes. The inclination of the impact angle increases the energy loss. The energy loss rate of the 45° impact is as high as 69.68%, of which 78% is generated by the impact-sliding stage. The normal force is mainly responsible for the wear removal and plastic deformation of Zr-4 alloy tubes. Tangential forces cause severe cutting in Zr-4 alloys and pushes the resulting wear debris away from the contact surfaces.