Remarkable Enhanced Mechanical Properties of TiAlCrNbV Medium-Entropy Alloy with Zr Additions
Most medium entropy alloys (MEAs) exhibit excellent mechanical properties, but their applications are limited because of their high density. This study explores a series of lightweight nonequiatomic Ti(65)(AlCrNbV)(35-x)Zr(x) (x = 3, 5, 7, and 10) MEAs with a low density, high strength, and high duc...
Autores principales: | , , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9506522/ https://www.ncbi.nlm.nih.gov/pubmed/36143635 http://dx.doi.org/10.3390/ma15186324 |
Sumario: | Most medium entropy alloys (MEAs) exhibit excellent mechanical properties, but their applications are limited because of their high density. This study explores a series of lightweight nonequiatomic Ti(65)(AlCrNbV)(35-x)Zr(x) (x = 3, 5, 7, and 10) MEAs with a low density, high strength, and high ductility. To achieve solid solution strengthening, Zr with a large atomic radius was used. In addition, various thermomechanical treatment parameters were adopted to further improve the MEAs’ mechanical properties. The density of the MEAs was revealed to be approximately 5 g/cm(3), indicating that they were lightweight. Through an X-ray diffraction analysis, the MEAs were revealed to have a single body-centered cubic structure not only in the as-cast state but also after thermomechanical treatment. In terms of mechanical properties, all the as-cast MEAs with Zr additions achieved excellent performance (>1000 MPa tensile yield strength and 20% tensile ductility). In addition, hot rolling effectively eliminated the defects of the MEAs; under a given yield strength, hot-rolled MEAs exhibited superior ductility relative to non-hot-rolled MEAs. Overall, the Ti(65)(AlCrNbV)(28)Zr(7) MEAs exhibited an optimum combination of mechanical properties (yield strength > 1200 MPa, plastic strain > 15%) after undergoing hot rolling 50%, cold rolling 70%, and rapid annealing for 30 to 50 s (at a temperature of approximately 850 °C) with a heating rate of 15 K/s. With their extremely high specific yield strength (264 MPa·g/cm(3)) and high ductility (22%), the Ti(65)(AlCrNbV)(28)Zr(7) MEAs demonstrate considerable potential for energy and transportation applications. |
---|