Cargando…

Effect of Metal-Cored Filler Wire on Surface Morphology and Micro-Hardness of Regulated Metal Deposition Welded ASTM A387-Gr.11-Cl.2 Steel Plates

Environmental and human-friendly welding is the need of the hour. In this context, this study explores the application of the regulated metal deposition (RMD) technique for ASTM A387-Gr.11-Cl.2 steel plates. To examine the effect of metal-cored filler wire (MCFW), MEGAFIL 237 M was employed during r...

Descripción completa

Detalles Bibliográficos
Autores principales: Bandhu, Din, Djavanroodi, Faramarz, Shaikshavali, G., Vora, Jay J., Abhishek, Kumar, Thakur, Ashish, Kumari, Soni, Saxena, Kuldeep K., Ebrahimi, Mahmoud, Attarilar, Shokouh
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9570648/
https://www.ncbi.nlm.nih.gov/pubmed/36234002
http://dx.doi.org/10.3390/ma15196661
_version_ 1784810162692816896
author Bandhu, Din
Djavanroodi, Faramarz
Shaikshavali, G.
Vora, Jay J.
Abhishek, Kumar
Thakur, Ashish
Kumari, Soni
Saxena, Kuldeep K.
Ebrahimi, Mahmoud
Attarilar, Shokouh
author_facet Bandhu, Din
Djavanroodi, Faramarz
Shaikshavali, G.
Vora, Jay J.
Abhishek, Kumar
Thakur, Ashish
Kumari, Soni
Saxena, Kuldeep K.
Ebrahimi, Mahmoud
Attarilar, Shokouh
author_sort Bandhu, Din
collection PubMed
description Environmental and human-friendly welding is the need of the hour. In this context, this study explores the application of the regulated metal deposition (RMD) technique for ASTM A387-Gr.11-Cl.2 steel plates. To examine the effect of metal-cored filler wire (MCFW), MEGAFIL 237 M was employed during regulated metal deposition (RMD) welding of 6 mm thick ASTM A387-Gr.11-Cl.2 steel plates. The welding was carried out at an optimized current (A) of 100 A, voltage (V) of 13 V, and gas flow rate (GFR) of 21 L/min. Thereafter, the as-welded plates were examined for morphological changes using optical microscopy. Additionally, the micro-hardness of the as-welded plates was measured to make corroboration with the obtained surface morphologies. In addition to this, the as-welded plates were subjected to heat treatment followed by surface morphology and micro-hardness examination. A comparison was made between the as-welded and heat-treated plates for their obtained surface morphologies and microhardness values. During this, it was observed that the weld zone of as-welded plates has a dendritic surface morphology which is very common in fusion-based welding. Similarly, the weld zone of heat-treated plates has a finer and erratic arrangement of martensite. Moreover, the obtained surface morphologies in the weld zone of as-welded and heat-treated plates have been justified by their respective hardness values of 1588.6 HV and 227.3 HV.
format Online
Article
Text
id pubmed-9570648
institution National Center for Biotechnology Information
language English
publishDate 2022
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-95706482022-10-17 Effect of Metal-Cored Filler Wire on Surface Morphology and Micro-Hardness of Regulated Metal Deposition Welded ASTM A387-Gr.11-Cl.2 Steel Plates Bandhu, Din Djavanroodi, Faramarz Shaikshavali, G. Vora, Jay J. Abhishek, Kumar Thakur, Ashish Kumari, Soni Saxena, Kuldeep K. Ebrahimi, Mahmoud Attarilar, Shokouh Materials (Basel) Article Environmental and human-friendly welding is the need of the hour. In this context, this study explores the application of the regulated metal deposition (RMD) technique for ASTM A387-Gr.11-Cl.2 steel plates. To examine the effect of metal-cored filler wire (MCFW), MEGAFIL 237 M was employed during regulated metal deposition (RMD) welding of 6 mm thick ASTM A387-Gr.11-Cl.2 steel plates. The welding was carried out at an optimized current (A) of 100 A, voltage (V) of 13 V, and gas flow rate (GFR) of 21 L/min. Thereafter, the as-welded plates were examined for morphological changes using optical microscopy. Additionally, the micro-hardness of the as-welded plates was measured to make corroboration with the obtained surface morphologies. In addition to this, the as-welded plates were subjected to heat treatment followed by surface morphology and micro-hardness examination. A comparison was made between the as-welded and heat-treated plates for their obtained surface morphologies and microhardness values. During this, it was observed that the weld zone of as-welded plates has a dendritic surface morphology which is very common in fusion-based welding. Similarly, the weld zone of heat-treated plates has a finer and erratic arrangement of martensite. Moreover, the obtained surface morphologies in the weld zone of as-welded and heat-treated plates have been justified by their respective hardness values of 1588.6 HV and 227.3 HV. MDPI 2022-09-26 /pmc/articles/PMC9570648/ /pubmed/36234002 http://dx.doi.org/10.3390/ma15196661 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Bandhu, Din
Djavanroodi, Faramarz
Shaikshavali, G.
Vora, Jay J.
Abhishek, Kumar
Thakur, Ashish
Kumari, Soni
Saxena, Kuldeep K.
Ebrahimi, Mahmoud
Attarilar, Shokouh
Effect of Metal-Cored Filler Wire on Surface Morphology and Micro-Hardness of Regulated Metal Deposition Welded ASTM A387-Gr.11-Cl.2 Steel Plates
title Effect of Metal-Cored Filler Wire on Surface Morphology and Micro-Hardness of Regulated Metal Deposition Welded ASTM A387-Gr.11-Cl.2 Steel Plates
title_full Effect of Metal-Cored Filler Wire on Surface Morphology and Micro-Hardness of Regulated Metal Deposition Welded ASTM A387-Gr.11-Cl.2 Steel Plates
title_fullStr Effect of Metal-Cored Filler Wire on Surface Morphology and Micro-Hardness of Regulated Metal Deposition Welded ASTM A387-Gr.11-Cl.2 Steel Plates
title_full_unstemmed Effect of Metal-Cored Filler Wire on Surface Morphology and Micro-Hardness of Regulated Metal Deposition Welded ASTM A387-Gr.11-Cl.2 Steel Plates
title_short Effect of Metal-Cored Filler Wire on Surface Morphology and Micro-Hardness of Regulated Metal Deposition Welded ASTM A387-Gr.11-Cl.2 Steel Plates
title_sort effect of metal-cored filler wire on surface morphology and micro-hardness of regulated metal deposition welded astm a387-gr.11-cl.2 steel plates
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9570648/
https://www.ncbi.nlm.nih.gov/pubmed/36234002
http://dx.doi.org/10.3390/ma15196661
work_keys_str_mv AT bandhudin effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates
AT djavanroodifaramarz effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates
AT shaikshavalig effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates
AT vorajayj effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates
AT abhishekkumar effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates
AT thakurashish effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates
AT kumarisoni effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates
AT saxenakuldeepk effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates
AT ebrahimimahmoud effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates
AT attarilarshokouh effectofmetalcoredfillerwireonsurfacemorphologyandmicrohardnessofregulatedmetaldepositionweldedastma387gr11cl2steelplates