Effect of Post-Weld Heat Treatment on Microstructure and Fracture Toughness of X80 Pipeline Steel Welded Joint
In the current study, post-weld heat treatment (PWHT 580 °C) was used for an X80 pipeline steel-welded joint, and the fracture toughness of the welded joint was investigated using a crack tip opening displacement (CTOD) test. The relationship between microstructure evolution and fracture toughness i...
Autores principales: | Wang, Xueli, Wang, Dongpo, Dai, Lianshuang, Deng, Caiyan, Li, Chengning, Wang, Yanjun, Shen, Ke |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9573030/ https://www.ncbi.nlm.nih.gov/pubmed/36233985 http://dx.doi.org/10.3390/ma15196646 |
Ejemplares similares
-
Effect of H(2)S Corrosion on the Fracture Toughness of the X80 Pipeline Steel Welded Joint
por: Wang, Xueli, et al.
Publicado: (2022) -
Statistical Assessment of Fracture Toughness Results from the HAZ of X80 Pipeline FCAW Girth Weld
por: Chen, Hongyuan, et al.
Publicado: (2022) -
Comparison of Fracture Toughness in the Coarse-Grain Heat-Affected Zone of X80 Pipelines Girth-Welded under Conventional and Ultra-Low Heat Input
por: Liu, Shuo, et al.
Publicado: (2022) -
Influence of Post-Weld Heat Treatment on Microstructure and Toughness Properties of 13MnNiMoR High Strength Low Alloy Steel Weld Joint
por: Tian, Songya, et al.
Publicado: (2021) -
Quantitative Correlation between Thermal Cycling and the Microstructures of X100 Pipeline Steel Laser-Welded Joints
por: Wang, Gang, et al.
Publicado: (2019)