Effect of Superhydrophobic Coating and Nanofiller Loading on Facial Elastomer Physical Properties
Facial prosthetics are currently constructed of materials that are far from optimal; superior materials with a “skin-like” feel are required. In this study, the property changes brought about by the consecutive additions of hydrophobic- and uncoated nano-SiO(2) to polydimethylsiloxane (PDMS) are ass...
Autores principales: | , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9610099/ https://www.ncbi.nlm.nih.gov/pubmed/36295406 http://dx.doi.org/10.3390/ma15207343 |
Sumario: | Facial prosthetics are currently constructed of materials that are far from optimal; superior materials with a “skin-like” feel are required. In this study, the property changes brought about by the consecutive additions of hydrophobic- and uncoated nano-SiO(2) to polydimethylsiloxane (PDMS) are assessed, and the alterations are compared with those observed for conventional submicron SiO(2)-filled materials. In sequence, 0%, 0.5%, 5%, 10%, and 15% by weight of each filler type were successively added to vinyl-terminated PDMS. Tensile, tear, Durometer hardness, translucency, and viscoelastic properties were assessed, and hardness and translucency were further measured after 3000 h of outdoor weathering. The results showed that 15% coated nano- SiO(2)-filled PDMS materials given the highest tensile strength, elastic modulus, storage modulus, loss modulus, tear strength, and durometer hardness (p < 0.05), whereas 15% submicron coated SiO(2)-filled materials displayed the highest failure strain and translucency parameter (p < 0.05). Only 10%- and 15%-filled submicron SiO(2) PDMS materials were altered by outdoor weathering; nevertheless, the increases were assessed to be too small to be clinically perceptible. As increased filler levels provided protection against solar radiation, heat, and moisture, only unfilled and 0.5%-filled PDMS formulations discolored from weathering. 15%-filled superhydrophobic-coated nano- SiO(2)-filled PDMS was found to produce the strongest, most tear-resistant, and least translucent materials, but it also produced materials with limited stretchability and high hardness, which were regarded to be downsides for creating a “skin-like” feel. |
---|