Cargando…

Effect of Graphene Oxide on the Properties of Polymer Inclusion Membranes for Gold Extraction from Acidic Solution

The cyanidation leaching method is hazardous to the environment, but it is widely applied in the gold mining process because it is effective for gold extraction. This study fabricates polymer inclusion membranes (PIMs), which have environment-friendly properties, with graphene oxide (GO) as an alter...

Descripción completa

Detalles Bibliográficos
Autores principales: Husna, Siti Madiha, Yusoff, Abdul Hafidz, Mohan, Mythili, Azmi, Nur Aina, Ter, Teo Pao, Shoparwe, Noor Fazliani, Sulaiman, Ahmad Ziad
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9611267/
https://www.ncbi.nlm.nih.gov/pubmed/36295755
http://dx.doi.org/10.3390/membranes12100996
Descripción
Sumario:The cyanidation leaching method is hazardous to the environment, but it is widely applied in the gold mining process because it is effective for gold extraction. This study fabricates polymer inclusion membranes (PIMs), which have environment-friendly properties, with graphene oxide (GO) as an alternative to the cyanidation leaching method for gold extraction. Poly(vinylidenefluoride-co-hexa-fluoropropylene)-based PIMs with different GO concentrations in five membranes (i.e., M1 (0 wt.%), M2 (0.5 wt.%), M3 (1.0 wt.%), M4 (1.5 wt.%), and M5 (2.0 wt.%)) are studied for their potential to extract gold from a hydrochloric acid solution. The membranes are prepared using di-(2-ethylhexyl) phosphoric acid as the extractant and dioctyl phthalate as the plasticizer. Scanning electron microscopy, Fourier-transform infrared spectroscopy, thermogravimetric analysis, ion exchange capacity, and water uptake are used to characterize the physical and chemical properties of the fabricated PIMs. The results show that the optimized membrane for gold extraction is M4 (1.5 wt.% GO), which yields a better performance on thermal stability, ion exchange capacity (IEC), and water uptake. M4 (1.5 wt.% GO) also exhibits a smooth and dense structure, with the maximum extraction efficiency obtained at 84.71% of extracted gold. In conclusion, PIMs can be used as an alternative for extracting gold with a better performance by the presence of 1.5 wt.% GO in membrane composition.