Cargando…

Adhesive Strength in Dentin Conditioned with 18% Ethylenediaminetetraacetic Acid versus 35% Phosphoric Acid: In Vitro Study with 1-Year Artificial Aging

The success and longevity of a resin composite restoration is determined by its good bonding to the tooth structure, with the adhesion being a challenge to dentin due to its complexity and structural heterogeneity. The present study aimed to compare the adhesive strength of dentin conditioned with 1...

Descripción completa

Detalles Bibliográficos
Autores principales: Alcántara-Obispo, Esther, Santander-Rengifo, Flor, Ladera-Castañeda, Marysela, López-Gurreonero, Carlos, Castro Pérez-Vargas, Antonieta, Cornejo-Pinto, Alberto, Cervantes-Ganoza, Luis, Cayo-Rojas, César
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9612237/
https://www.ncbi.nlm.nih.gov/pubmed/36297869
http://dx.doi.org/10.3390/polym14204291
Descripción
Sumario:The success and longevity of a resin composite restoration is determined by its good bonding to the tooth structure, with the adhesion being a challenge to dentin due to its complexity and structural heterogeneity. The present study aimed to compare the adhesive strength of dentin conditioned with 18% ethylenediaminetetraacetic acid (EDTA) versus 35% phosphoric acid (H(3)PO(4)) in human premolars. Materials and Methods: This in vitro experimental study was performed on 40 human premolars. The occlusal thirds were sectioned and randomly placed into four groups according to the type of dentin conditioning: Group 1 (control), Group 2 (18% EDTA), Group 3 (35% H(3)PO(4)) and Group 4 (18% EDTA plus 35% H(3)PO(4)). Then, 10,000 thermocycles between 5 +/− 2 °C and 55 +/− 2 °C were applied. Adhesive strength was tested by shearing with a digital universal testing machine at a crosshead speed of 0.75 mm/min. The values obtained were analyzed in megapascals (MPa). The mean and standard deviation were used as measures of central tendency and dispersion. In addition, a one-factor intergroup ANOVA test was applied with Tukey’s post hoc test considering a significance level of p < 0.05. Results: The 18% EDTA and 18% EDTA plus 35% H(3)PO(4) showed significantly higher adhesive strength compared to the control group that did not receive dentin conditioning (p = 0.047 and p < 0.001, respectively). However, the group conditioned with 18% EDTA did not present significant differences compared to the group conditioned with 35% H(3)PO(4) (p = 0.997). In addition, the group conditioned with 18% EDTA plus 35% H(3)PO(4) showed significantly higher adhesive strength compared to the groups conditioned with 18% EDTA (p = 0.002) and 35% H(3)PO(4) (p = 0.001). Conclusion: The adhesion of bulk fill resin composite to dentin was favorable when preconditioning was performed using 18% EDTA followed by 35% H(3)PO(4). In contrast, when both etchants were used separately, the bulk fill resin composite showed similar bond strength values in both cases, but significantly lower compared to their sequential application.