Ultrafast-Laser Micro-Structuring of LiNi(0.8)Mn(0.1)Co(0.1)O(2) Cathode for High-Rate Capability of Three-Dimensional Li-ion Batteries

Femtosecond ultrafast-laser micro-patterning was employed to prepare a three-dimensional (3D) structure for the tape-casting Ni-rich LiNi(0.8)Mn(0.1)Co(0.1)O(2) (NMC811) cathode. The influences of laser structuring on the electrochemical performance of NMC811 were investigated. The 3D-NMC811 cathode...

Descripción completa

Detalles Bibliográficos
Autores principales: Tran, Minh Xuan, Smyrek, Peter, Park, Jihun, Pfleging, Wilhelm, Lee, Joong Kee
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9654857/
https://www.ncbi.nlm.nih.gov/pubmed/36364674
http://dx.doi.org/10.3390/nano12213897
Descripción
Sumario:Femtosecond ultrafast-laser micro-patterning was employed to prepare a three-dimensional (3D) structure for the tape-casting Ni-rich LiNi(0.8)Mn(0.1)Co(0.1)O(2) (NMC811) cathode. The influences of laser structuring on the electrochemical performance of NMC811 were investigated. The 3D-NMC811 cathode retained capacities of 77.8% at 2 C of initial capacity at 0.1 C, which was thrice that of 2D-NMC811 with an initial capacity of 27.8%. Cyclic voltammetry (CV) and impedance spectroscopy demonstrated that the 3D electrode improved the Li(+) ion transportation at the electrode–electrolyte interface, resulting in a higher rate capability. The diffusivity coefficient D(Li+), calculated by both CV and electrochemical impedance spectroscopy, revealed that 3D-NMC811 delivered faster Li(+) ion transportation with higher D(Li+) than that of 2D-NMC811. The laser ablation of the active material also led to a lower charge–transfer resistance, which represented lower polarization and improved Li(+) ion diffusivity.