Factory Crystallized Silicates for Monolithic Metal-Free Restorations: A Flexural Strength and Translucency Comparison Test
Flexural strength (FS) and translucency (Contrast Ratio-CR) of three different factory crystallized silica-based glass ceramics, Celtra Duo (CD), N!ce (NI) and Li-Si Block, a lithium disilicate, IPS e.max CAD (LD), and a leucite-reinforced feldspathic ceramic, Empress CAD (EM), in two different tran...
Autores principales: | Vichi, Alessandro, Zhao, Zejiao, Paolone, Gaetano, Scotti, Nicola, Mutahar, Mahdi, Goracci, Cecilia, Louca, Chris |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9657079/ https://www.ncbi.nlm.nih.gov/pubmed/36363425 http://dx.doi.org/10.3390/ma15217834 |
Ejemplares similares
-
Translucency of Lithium-Based Silicate Glass–Ceramics Blocks for CAD/CAM Procedures: A Narrative Review
por: Vichi, Alessandro, et al.
Publicado: (2023) -
Flexural Strength of CAD/CAM Lithium-Based Silicate Glass–Ceramics: A Narrative Review
por: Munoz, Alvaro, et al.
Publicado: (2023) -
Translucency of CAD/CAM and 3D Printable Composite Materials for Permanent Dental Restorations
por: Vichi, Alessandro, et al.
Publicado: (2023) -
Effect of different sintering process on flexural strength of translucency monolithic zirconia
por: Juntavee, Niwut, et al.
Publicado: (2018) -
The Effect of Translucency and Surface Treatment on the Flexural Strength of Aged Monolithic Zirconia
por: Giti, Rashin, et al.
Publicado: (2021)