Cargando…
Shear Bond Strength of Polypropylene Fiber in Orthodontic Adhesive on Glazed Monolithic Zirconia
This study aims to compare shear bond strength (SBS) and mode of failure (MOF) between ceramic and metal orthodontic brackets on glazed monolithic zirconia using non-woven polypropylene fiber adhesive. Sixty glazed and sintered zirconia blocks were divided into six groups and attached with orthodont...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9658274/ https://www.ncbi.nlm.nih.gov/pubmed/36365620 http://dx.doi.org/10.3390/polym14214627 |
_version_ | 1784829910825566208 |
---|---|
author | Riowruangsanggoon, Dhanabhol Riddhabhaya, Apiwat Niyomtham, Nattisa Sirisoontorn, Irin |
author_facet | Riowruangsanggoon, Dhanabhol Riddhabhaya, Apiwat Niyomtham, Nattisa Sirisoontorn, Irin |
author_sort | Riowruangsanggoon, Dhanabhol |
collection | PubMed |
description | This study aims to compare shear bond strength (SBS) and mode of failure (MOF) between ceramic and metal orthodontic brackets on glazed monolithic zirconia using non-woven polypropylene fiber adhesive. Sixty glazed and sintered zirconia blocks were divided into six groups and attached with orthodontic brackets as follows: CS, ceramic bracket with silane; CB, ceramic bracket with bonding agent; CBS, ceramic bracket with bonding agent and silane; MS, metal bracket with silane; MB, metal bracket with bonding agent; and MBS, metal bracket with bonding agent and silane. There was a statistically significant difference in mean SBS values (p < 0.001). The CS group showed the highest SBS value (23.42 ± 3.88 MPa). On the other hand, the lowest was found in the MB group, which was not statistically different from the CB group (3.26 ± 0.76 and 5.09 ± 1.50 MPa, respectively). The MS, MBS, and CBS groups showed no statistical difference compared to each other (15.57 ± 4.01, 13.23 ± 5.47, and 12.77 ± 4.43 MPa, respectively). SBS is highest when a ceramic bracket with silane is bonded to glazed monolithic zirconia. |
format | Online Article Text |
id | pubmed-9658274 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2022 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-96582742022-11-15 Shear Bond Strength of Polypropylene Fiber in Orthodontic Adhesive on Glazed Monolithic Zirconia Riowruangsanggoon, Dhanabhol Riddhabhaya, Apiwat Niyomtham, Nattisa Sirisoontorn, Irin Polymers (Basel) Article This study aims to compare shear bond strength (SBS) and mode of failure (MOF) between ceramic and metal orthodontic brackets on glazed monolithic zirconia using non-woven polypropylene fiber adhesive. Sixty glazed and sintered zirconia blocks were divided into six groups and attached with orthodontic brackets as follows: CS, ceramic bracket with silane; CB, ceramic bracket with bonding agent; CBS, ceramic bracket with bonding agent and silane; MS, metal bracket with silane; MB, metal bracket with bonding agent; and MBS, metal bracket with bonding agent and silane. There was a statistically significant difference in mean SBS values (p < 0.001). The CS group showed the highest SBS value (23.42 ± 3.88 MPa). On the other hand, the lowest was found in the MB group, which was not statistically different from the CB group (3.26 ± 0.76 and 5.09 ± 1.50 MPa, respectively). The MS, MBS, and CBS groups showed no statistical difference compared to each other (15.57 ± 4.01, 13.23 ± 5.47, and 12.77 ± 4.43 MPa, respectively). SBS is highest when a ceramic bracket with silane is bonded to glazed monolithic zirconia. MDPI 2022-10-31 /pmc/articles/PMC9658274/ /pubmed/36365620 http://dx.doi.org/10.3390/polym14214627 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Riowruangsanggoon, Dhanabhol Riddhabhaya, Apiwat Niyomtham, Nattisa Sirisoontorn, Irin Shear Bond Strength of Polypropylene Fiber in Orthodontic Adhesive on Glazed Monolithic Zirconia |
title | Shear Bond Strength of Polypropylene Fiber in Orthodontic Adhesive on Glazed Monolithic Zirconia |
title_full | Shear Bond Strength of Polypropylene Fiber in Orthodontic Adhesive on Glazed Monolithic Zirconia |
title_fullStr | Shear Bond Strength of Polypropylene Fiber in Orthodontic Adhesive on Glazed Monolithic Zirconia |
title_full_unstemmed | Shear Bond Strength of Polypropylene Fiber in Orthodontic Adhesive on Glazed Monolithic Zirconia |
title_short | Shear Bond Strength of Polypropylene Fiber in Orthodontic Adhesive on Glazed Monolithic Zirconia |
title_sort | shear bond strength of polypropylene fiber in orthodontic adhesive on glazed monolithic zirconia |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9658274/ https://www.ncbi.nlm.nih.gov/pubmed/36365620 http://dx.doi.org/10.3390/polym14214627 |
work_keys_str_mv | AT riowruangsanggoondhanabhol shearbondstrengthofpolypropylenefiberinorthodonticadhesiveonglazedmonolithiczirconia AT riddhabhayaapiwat shearbondstrengthofpolypropylenefiberinorthodonticadhesiveonglazedmonolithiczirconia AT niyomthamnattisa shearbondstrengthofpolypropylenefiberinorthodonticadhesiveonglazedmonolithiczirconia AT sirisoontornirin shearbondstrengthofpolypropylenefiberinorthodonticadhesiveonglazedmonolithiczirconia |