Cargando…

Micromechanical Deformation Processes and Failure of PBS Based Composites Containing Ultra-Short Cellulosic Fibers for Injection Molding Applications

The use of biobased thermoplastic polymers has gained great attention in the last years as a potential alternative to fossil-based thermoplastic polymers. Biobased polymers in fact offer advantages not only in terms of reduced dependence on fossil resources but they also lower the CO(2) footprint in...

Descripción completa

Detalles Bibliográficos
Autores principales: Aliotta, Laura, Gasenge, Mattia, Gigante, Vito, Lazzeri, Andrea
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9658727/
https://www.ncbi.nlm.nih.gov/pubmed/36365493
http://dx.doi.org/10.3390/polym14214499
Descripción
Sumario:The use of biobased thermoplastic polymers has gained great attention in the last years as a potential alternative to fossil-based thermoplastic polymers. Biobased polymers in fact offer advantages not only in terms of reduced dependence on fossil resources but they also lower the CO(2) footprint in accordance with sustainability and climate protection goals. To improve the properties of these materials, reinforcement with biobased fibers is a promising solution; however, it must be kept in mind that the fibers aspect ratio and the interfacial adhesion between the reinforcement and the matrix plays an important role influencing both physical and mechanical properties of the biocomposites. In this paper, the possibility of producing composites by injection molding, based on polybutylene succinate and ultra-short cellulosic fibers has been explored as a potential biobased solution. Thermo-mechanical properties of the composites were investigated, paying particular attention to the local micromechanical deformation processes, investigated by dilatometric tests, and failure mechanisms. Analytical models were also applied to predict the elastic and flexural modulus and the interfacial properties of the biocomposites. Good results were achieved, demonstrating the that this class of biocomposite can be exploited. Compared to pure PBS, the composites with 30 wt.% of cellulose fibers increased the Young’s modulus by 154%, the flexural modulus by 130% and the heat deflection temperature by 9%.