Synthesis of Biobased Hydroxyl-Terminated Oligomers by Metathesis Degradation of Industrial Rubbers SBS and PB: Tailor-Made Unsaturated Diols and Polyols

Biobased hydroxyl-terminated polybutadiene (HTPB) was successfully synthesized in a one-pot reaction via metathesis degradation of industrial rubbers. Thus, polybutadiene (PB) and poly(styrene-butadiene-styrene) (SBS) were degraded via metathesis with high yields (>94%), using the fatty alcohol 1...

Descripción completa

Detalles Bibliográficos
Autores principales: Burelo, Manuel, Gutiérrez, Selena, Treviño-Quintanilla, Cecilia D., Cruz-Morales, Jorge A., Martínez, Araceli, López-Morales, Salvador
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9692933/
https://www.ncbi.nlm.nih.gov/pubmed/36433100
http://dx.doi.org/10.3390/polym14224973
_version_ 1784837400182128640
author Burelo, Manuel
Gutiérrez, Selena
Treviño-Quintanilla, Cecilia D.
Cruz-Morales, Jorge A.
Martínez, Araceli
López-Morales, Salvador
author_facet Burelo, Manuel
Gutiérrez, Selena
Treviño-Quintanilla, Cecilia D.
Cruz-Morales, Jorge A.
Martínez, Araceli
López-Morales, Salvador
author_sort Burelo, Manuel
collection PubMed
description Biobased hydroxyl-terminated polybutadiene (HTPB) was successfully synthesized in a one-pot reaction via metathesis degradation of industrial rubbers. Thus, polybutadiene (PB) and poly(styrene-butadiene-styrene) (SBS) were degraded via metathesis with high yields (>94%), using the fatty alcohol 10-undecen-1-ol as a chain transfer agent (CTA) and the second-generation Grubbs–Hoveyda catalyst. The identification of the hydroxyl groups (-OH) and the formation of biobased HTPB were verified by FT-IR and NMR. Likewise, the molecular weight and properties of the HTPB were controlled by changing the molar ratio of rubber to CTA ([C=C]/CTA) from 1:1 to 100:1, considering a constant molar ratio of the catalyst ([C=C]/Ru = 500:1). The number average molecular weight (M(n)) ranged between 583 and 6580 g/mol and the decomposition temperatures between 134 and 220 °C. Moreover, the catalyst optimization study showed that at catalyst loadings as low as [C=C]/Ru = 5000:1, the theoretical molecular weight is in good agreement with the experimental molecular weight and the expected diols and polyols are formed. At higher ratios than those, the difference between theoretical and experimental molecular weight is wide, and there is no control over HTPB. Therefore, the rubber/CTA molar ratio and the amount of catalyst play an important role in PB degradation and HTPB synthesis. Biobased HTPB can be used to synthesize engineering design polymers, intermediates, fine chemicals, and in the polyurethane industry, and contribute to the development of environmentally friendly raw materials.
format Online
Article
Text
id pubmed-9692933
institution National Center for Biotechnology Information
language English
publishDate 2022
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-96929332022-11-26 Synthesis of Biobased Hydroxyl-Terminated Oligomers by Metathesis Degradation of Industrial Rubbers SBS and PB: Tailor-Made Unsaturated Diols and Polyols Burelo, Manuel Gutiérrez, Selena Treviño-Quintanilla, Cecilia D. Cruz-Morales, Jorge A. Martínez, Araceli López-Morales, Salvador Polymers (Basel) Article Biobased hydroxyl-terminated polybutadiene (HTPB) was successfully synthesized in a one-pot reaction via metathesis degradation of industrial rubbers. Thus, polybutadiene (PB) and poly(styrene-butadiene-styrene) (SBS) were degraded via metathesis with high yields (>94%), using the fatty alcohol 10-undecen-1-ol as a chain transfer agent (CTA) and the second-generation Grubbs–Hoveyda catalyst. The identification of the hydroxyl groups (-OH) and the formation of biobased HTPB were verified by FT-IR and NMR. Likewise, the molecular weight and properties of the HTPB were controlled by changing the molar ratio of rubber to CTA ([C=C]/CTA) from 1:1 to 100:1, considering a constant molar ratio of the catalyst ([C=C]/Ru = 500:1). The number average molecular weight (M(n)) ranged between 583 and 6580 g/mol and the decomposition temperatures between 134 and 220 °C. Moreover, the catalyst optimization study showed that at catalyst loadings as low as [C=C]/Ru = 5000:1, the theoretical molecular weight is in good agreement with the experimental molecular weight and the expected diols and polyols are formed. At higher ratios than those, the difference between theoretical and experimental molecular weight is wide, and there is no control over HTPB. Therefore, the rubber/CTA molar ratio and the amount of catalyst play an important role in PB degradation and HTPB synthesis. Biobased HTPB can be used to synthesize engineering design polymers, intermediates, fine chemicals, and in the polyurethane industry, and contribute to the development of environmentally friendly raw materials. MDPI 2022-11-17 /pmc/articles/PMC9692933/ /pubmed/36433100 http://dx.doi.org/10.3390/polym14224973 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Burelo, Manuel
Gutiérrez, Selena
Treviño-Quintanilla, Cecilia D.
Cruz-Morales, Jorge A.
Martínez, Araceli
López-Morales, Salvador
Synthesis of Biobased Hydroxyl-Terminated Oligomers by Metathesis Degradation of Industrial Rubbers SBS and PB: Tailor-Made Unsaturated Diols and Polyols
title Synthesis of Biobased Hydroxyl-Terminated Oligomers by Metathesis Degradation of Industrial Rubbers SBS and PB: Tailor-Made Unsaturated Diols and Polyols
title_full Synthesis of Biobased Hydroxyl-Terminated Oligomers by Metathesis Degradation of Industrial Rubbers SBS and PB: Tailor-Made Unsaturated Diols and Polyols
title_fullStr Synthesis of Biobased Hydroxyl-Terminated Oligomers by Metathesis Degradation of Industrial Rubbers SBS and PB: Tailor-Made Unsaturated Diols and Polyols
title_full_unstemmed Synthesis of Biobased Hydroxyl-Terminated Oligomers by Metathesis Degradation of Industrial Rubbers SBS and PB: Tailor-Made Unsaturated Diols and Polyols
title_short Synthesis of Biobased Hydroxyl-Terminated Oligomers by Metathesis Degradation of Industrial Rubbers SBS and PB: Tailor-Made Unsaturated Diols and Polyols
title_sort synthesis of biobased hydroxyl-terminated oligomers by metathesis degradation of industrial rubbers sbs and pb: tailor-made unsaturated diols and polyols
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9692933/
https://www.ncbi.nlm.nih.gov/pubmed/36433100
http://dx.doi.org/10.3390/polym14224973
work_keys_str_mv AT burelomanuel synthesisofbiobasedhydroxylterminatedoligomersbymetathesisdegradationofindustrialrubberssbsandpbtailormadeunsaturateddiolsandpolyols
AT gutierrezselena synthesisofbiobasedhydroxylterminatedoligomersbymetathesisdegradationofindustrialrubberssbsandpbtailormadeunsaturateddiolsandpolyols
AT trevinoquintanillaceciliad synthesisofbiobasedhydroxylterminatedoligomersbymetathesisdegradationofindustrialrubberssbsandpbtailormadeunsaturateddiolsandpolyols
AT cruzmoralesjorgea synthesisofbiobasedhydroxylterminatedoligomersbymetathesisdegradationofindustrialrubberssbsandpbtailormadeunsaturateddiolsandpolyols
AT martinezaraceli synthesisofbiobasedhydroxylterminatedoligomersbymetathesisdegradationofindustrialrubberssbsandpbtailormadeunsaturateddiolsandpolyols
AT lopezmoralessalvador synthesisofbiobasedhydroxylterminatedoligomersbymetathesisdegradationofindustrialrubberssbsandpbtailormadeunsaturateddiolsandpolyols