Cargando…
Cu Nanowires and Nanoporous Ag Matrix Fabricated through Directional Solidification and Selective Dissolution of Ag–Cu Eutectic Alloys
Cu nanowires and a nanoporous Ag matrix were fabricated through directional solidification and selective dissolution of Ag–Cu eutectic alloys. Ag-39.9at.%Cu eutectic alloys were directionally solidified at growth rates of 14, 25, and 34 μm/s at a temperature gradient of 10 K/cm. The Cu phase in the...
Autores principales: | Xu, Jiaxing, Gao, Jianjun, Qin, Hongling, Liu, Zhiyang, Zhu, Linpeng, Geng, Haibin, Yao, Ligang, Zhao, Zhilong |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9698229/ https://www.ncbi.nlm.nih.gov/pubmed/36431677 http://dx.doi.org/10.3390/ma15228189 |
Ejemplares similares
-
Dissolution of Ag Precipitates in the Cu–8wt.%Ag Alloy Deformed by High Pressure Torsion
por: Korneva, Anna, et al.
Publicado: (2019) -
Fabrication and Characteristics of SnAgCu Alloy Nanowires for Electrical Connection Application
por: Chen, Jung-Hsuan, et al.
Publicado: (2018) -
Effects of an Alternating Magnetic Field/Ag Multi-Alloying Combined Solidification Process on Cu–14Fe Alloy
por: Zou, Jin, et al.
Publicado: (2018) -
The Effects of Adding Elements of Zinc and Magnesium on Ag-Cu Eutectic Alloy for Warming Acupuncture
por: Kim, Yu Kyoung, et al.
Publicado: (2013) -
The Effect of Cu:Ag Atomic Ratio on the Properties of Sputtered Cu–Ag Alloy Thin Films
por: Hsieh, Janghsing, et al.
Publicado: (2016)