Comparative Measurements and Analysis of the Electrical Properties of Nanocomposites Ti(x)Zr(1−x)C+α-Cy (0.0 ≤ x ≤ 1.0)
In this paper, the frequency-temperature dependence of the conductivity and dielectric permittivity of nc-Ti(x)Zr(1−)(x)C+α-C(y) (0.0 ≤ x ≤ 1.0) nanocomposites produced by dual-source magnetron sputtering was determined. The films produced are biphasic layers with an excess of amorphous carbon relat...
Autores principales: | , , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9698743/ https://www.ncbi.nlm.nih.gov/pubmed/36431391 http://dx.doi.org/10.3390/ma15227908 |
Sumario: | In this paper, the frequency-temperature dependence of the conductivity and dielectric permittivity of nc-Ti(x)Zr(1−)(x)C+α-C(y) (0.0 ≤ x ≤ 1.0) nanocomposites produced by dual-source magnetron sputtering was determined. The films produced are biphasic layers with an excess of amorphous carbon relative to the stoichiometric composition of Ti(x)Zr(1−x)C. The matrix was amorphous carbon, and the dispersed phase was carbide nanoparticles. AC measurements were performed in the frequency range of 50 Hz–5 MHz at temperatures from 20 K to 373 K. It was found that both conductivity and permittivity relationships are determined by three tunneling mechanisms, differing in relaxation times. The maxima in the low- and high-frequency regions decrease with increasing temperature. The maximum in the mid-frequency region increases with increasing temperature. The low-frequency maximum is due to electron tunneling between the carbon films on the surface of the carbide nanoshells. The mid-frequency maximum is due to electron transitions between the nano size grains. The high-frequency maximum is associated with tunneling between the nano-grains and the carbon shells. It has been established that dipole relaxation occurs in the nanocomposites according to the Cole-Cole mechanism. The increase in static dielectric permittivity with increasing measurement temperature is indicative of a step polarisation mechanism. In the frequency region above 1 MHz, anomalous dispersion—an increase in permittivity with increasing frequency—was observed for all nanocomposite contents. |
---|