On Comparison of Heat Treated and Non-Heat-Treated LOM Manufactured Sample for Poly(lactic)acid: Mechanical and Morphological View Point

This work reports the comparison of heat-treated and non-heat-treated laminated object-manufactured (LOM) 3D-printed specimens from mechanical and morphological viewpoints. The study suggests that heat treatment of the FDM-printed specimen may have a significant impact on the material characteristic...

Descripción completa

Detalles Bibliográficos
Autores principales: Singh, I., Kumar, S., R. Koloor, S. S., Kumar, D., Yahya, M. Y., Mago, J.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9737080/
https://www.ncbi.nlm.nih.gov/pubmed/36501501
http://dx.doi.org/10.3390/polym14235098
Descripción
Sumario:This work reports the comparison of heat-treated and non-heat-treated laminated object-manufactured (LOM) 3D-printed specimens from mechanical and morphological viewpoints. The study suggests that heat treatment of the FDM-printed specimen may have a significant impact on the material characteristics of the polymer. The work has been performed at two stages for the characterization of (a) non-heat-treated samples and (b) heat-treated samples. The results for stage 1 (non-heat-treated samples) suggest that the infill density: 70%, infill pattern: honeycomb, and six number of discs in a single LOM-manufactured sample is the optimized condition with a compression strength of 42.47 MPa. The heat treatment analysis at stage 2 suggests that a high temperature: 65 °C, low time interval: 10 min, works equally well as the low temperature: 55 °C, high time interval: 30 min. The post-heat treatment near Tg (65 °C) for a time interval of 10 min improved the compressive strength by 105.42%.