Role of ZnO Nanoparticles Loading in Modifying the Morphological, Optical, and Thermal Properties of Immiscible Polymer (PMMA/PEG) Blends

High-performance hybrid polymer blends can be prepared by blending different types of polymers to improve their properties. However, most polymer blends exhibit phase separation after blending. In this study, polymethylmethacrylate/polyethylene glycol (PMMA/PEG) polymer blends (70/30 and 30/70 w/w)...

Descripción completa

Detalles Bibliográficos
Autores principales: Hammani, Salim, Daikhi, Sihem, Bechelany, Mikhael, Barhoum, Ahmed
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9738493/
https://www.ncbi.nlm.nih.gov/pubmed/36499948
http://dx.doi.org/10.3390/ma15238453
Descripción
Sumario:High-performance hybrid polymer blends can be prepared by blending different types of polymers to improve their properties. However, most polymer blends exhibit phase separation after blending. In this study, polymethylmethacrylate/polyethylene glycol (PMMA/PEG) polymer blends (70/30 and 30/70 w/w) were prepared by solution casting with and without ZnO nanoparticles (NPs) loading. The effect of loading ZnO nanoparticles on blend morphology, UV blocking, glass transition, melting, and crystallization were investigated. Without loading ZnO NP, the PMMA/PEG blends showed phase separation, especially the PEG-rich blend. Loading PMMA/PEG blend with ZnO NPs increased the miscibility of the blend and most of the ZnO NPs dispersed in the PEG phase. The interaction of the ZnO NPs with the blend polymers slightly decreased the intensity of infrared absorption of the functional groups. The UV-blocking properties of the blends increased by 15% and 20%, and the band gap energy values were 4.1 eV and 3.8 eV for the blends loaded with ZnO NPs with a PMMA/PEG ratio of 70/30 and 30/70, respectively. In addition, the glass transition temperature (T(g)) increased by 14 °C, the crystallinity rate increased by 15%, the melting (T(m)) and crystallization(T(c)) temperatures increased by 2 °C and 14 °C, respectively, and the thermal stability increased by 25 °C compared to the PMMA/PEG blends without ZnO NP loading.