Effect of Complex Strengthening on the Continuous Cooling Transformation Behavior of High-Strength Rebar
The effects of niobium and composite strengthening on the phase transformation characteristics and precipitation behavior of continuous cooling transformation of high-strength rebar during thermal deformation and subsequent cooling were investigated. The results show that when the cooling rate was w...
Autores principales: | , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9780884/ https://www.ncbi.nlm.nih.gov/pubmed/36556745 http://dx.doi.org/10.3390/ma15248940 |
_version_ | 1784856938222190592 |
---|---|
author | You, Jingtian Li, Zhiying Wang, Jie Li, Changrong Zeng, Zeyun Li, Shiwang Huang, Sheng |
author_facet | You, Jingtian Li, Zhiying Wang, Jie Li, Changrong Zeng, Zeyun Li, Shiwang Huang, Sheng |
author_sort | You, Jingtian |
collection | PubMed |
description | The effects of niobium and composite strengthening on the phase transformation characteristics and precipitation behavior of continuous cooling transformation of high-strength rebar during thermal deformation and subsequent cooling were investigated. The results show that when the cooling rate was within 0.3–5 °C/s, ferrite transformation and pearlite transformation occurred in the experimental steels. The Nb content increased to 0.062 wt.%, and the starting temperature of the ferrite transformation decreased. Meanwhile, the ferrite phase transformation zone gradually expanded, and the pearlite phase transformation zone gradually narrowed with the increase in the cooling rate. When the cooling rate was 1 °C/s, bainite transformation began to occur, and the amount of transformation increased with the increase in the cooling rate. It was found that the main precipitates in the experimental steels were (Nb, Ti, V)C, with an average particle size of about 10–50 nm. When the Nb content was increased to 0.062 wt.% and the cooling rate was increased to 5 °C/s, the ferrite grain size was reduced from 19.5 to 7.5 μm, and the particle size of the precipitate (Nb, Ti, V)C could be effectively reduced. The strength of the steel was significantly improved, but the elongation of the steel was reduced. However, the comprehensive mechanical properties of 0.062 wt.% Nb experimental steel was significantly improved at a cooling rate of 5 °C/s. |
format | Online Article Text |
id | pubmed-9780884 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2022 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-97808842022-12-24 Effect of Complex Strengthening on the Continuous Cooling Transformation Behavior of High-Strength Rebar You, Jingtian Li, Zhiying Wang, Jie Li, Changrong Zeng, Zeyun Li, Shiwang Huang, Sheng Materials (Basel) Article The effects of niobium and composite strengthening on the phase transformation characteristics and precipitation behavior of continuous cooling transformation of high-strength rebar during thermal deformation and subsequent cooling were investigated. The results show that when the cooling rate was within 0.3–5 °C/s, ferrite transformation and pearlite transformation occurred in the experimental steels. The Nb content increased to 0.062 wt.%, and the starting temperature of the ferrite transformation decreased. Meanwhile, the ferrite phase transformation zone gradually expanded, and the pearlite phase transformation zone gradually narrowed with the increase in the cooling rate. When the cooling rate was 1 °C/s, bainite transformation began to occur, and the amount of transformation increased with the increase in the cooling rate. It was found that the main precipitates in the experimental steels were (Nb, Ti, V)C, with an average particle size of about 10–50 nm. When the Nb content was increased to 0.062 wt.% and the cooling rate was increased to 5 °C/s, the ferrite grain size was reduced from 19.5 to 7.5 μm, and the particle size of the precipitate (Nb, Ti, V)C could be effectively reduced. The strength of the steel was significantly improved, but the elongation of the steel was reduced. However, the comprehensive mechanical properties of 0.062 wt.% Nb experimental steel was significantly improved at a cooling rate of 5 °C/s. MDPI 2022-12-14 /pmc/articles/PMC9780884/ /pubmed/36556745 http://dx.doi.org/10.3390/ma15248940 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article You, Jingtian Li, Zhiying Wang, Jie Li, Changrong Zeng, Zeyun Li, Shiwang Huang, Sheng Effect of Complex Strengthening on the Continuous Cooling Transformation Behavior of High-Strength Rebar |
title | Effect of Complex Strengthening on the Continuous Cooling Transformation Behavior of High-Strength Rebar |
title_full | Effect of Complex Strengthening on the Continuous Cooling Transformation Behavior of High-Strength Rebar |
title_fullStr | Effect of Complex Strengthening on the Continuous Cooling Transformation Behavior of High-Strength Rebar |
title_full_unstemmed | Effect of Complex Strengthening on the Continuous Cooling Transformation Behavior of High-Strength Rebar |
title_short | Effect of Complex Strengthening on the Continuous Cooling Transformation Behavior of High-Strength Rebar |
title_sort | effect of complex strengthening on the continuous cooling transformation behavior of high-strength rebar |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9780884/ https://www.ncbi.nlm.nih.gov/pubmed/36556745 http://dx.doi.org/10.3390/ma15248940 |
work_keys_str_mv | AT youjingtian effectofcomplexstrengtheningonthecontinuouscoolingtransformationbehaviorofhighstrengthrebar AT lizhiying effectofcomplexstrengtheningonthecontinuouscoolingtransformationbehaviorofhighstrengthrebar AT wangjie effectofcomplexstrengtheningonthecontinuouscoolingtransformationbehaviorofhighstrengthrebar AT lichangrong effectofcomplexstrengtheningonthecontinuouscoolingtransformationbehaviorofhighstrengthrebar AT zengzeyun effectofcomplexstrengtheningonthecontinuouscoolingtransformationbehaviorofhighstrengthrebar AT lishiwang effectofcomplexstrengtheningonthecontinuouscoolingtransformationbehaviorofhighstrengthrebar AT huangsheng effectofcomplexstrengtheningonthecontinuouscoolingtransformationbehaviorofhighstrengthrebar |