Effect of Temperature Cycling Pretreatment on the Thermal Stability of Sm(2)(Co, Fe, Zr, Cu)(17) Magnets in the Mild Temperature Range

The irredeemable magnetic losses of Sm(Co, Fe, Zr, Cu)(7.8) permanent magnets caused by oxidation are very important for their practical application. In this work, the simulated results with R(2) ≥ 98% based on the data of the temperature cycling test and the long-term isothermal test for the origin...