On the Use of Multi-Step Dies for Improving the Performance against Hydrogen Embrittlement of Cold Drawn Prestressing Steel Wires
The main cause of in-service failure of cold drawn wires in aggressive environments is hydrogen embrittlement (HE). The non-uniform plastic strains and residual stresses generated after cold drawing play a significant role in the matter of HE susceptibility of prestressing steels. In this paper, a n...
Autores principales: | Toribio, Jesús, Lorenzo, Miguel |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9785074/ https://www.ncbi.nlm.nih.gov/pubmed/36556889 http://dx.doi.org/10.3390/ma15249085 |
Ejemplares similares
-
Analysis of Fatigue Crack Paths in Cold Drawn Pearlitic Steel
por: Toribio, Jesús, et al.
Publicado: (2015) -
Influence of Residual Stress Field on the Fatigue Crack Propagation in Prestressing Steel Wires
por: Toribio, Jesús, et al.
Publicado: (2015) -
Innovative Design of Residual Stress and Strain Distributions for Analyzing the Hydrogen Embrittlement Phenomenon in Metallic Materials
por: Toribio, Jesús, et al.
Publicado: (2022) -
Quantification of Temperature Dependence of Hydrogen Embrittlement in Pipeline Steel
por: Xing, Xiao, et al.
Publicado: (2019) -
Hydrogen Uptake and Embrittlement of Carbon Steels in Various Environments
por: Trautmann, Anton, et al.
Publicado: (2020)