A Novel Parameter for Fatigue Damage Assessment of Laser-Repaired Nickel-Based Alloy

The fatigue damage assessment of laser-repaired components is critical to their service safety. However, since laser repairing is an advanced green remanufacturing technology, the current research on its fatigue mechanical behavior and fatigue damage evaluation methods is still immature. In addition...

Descripción completa

Detalles Bibliográficos
Autores principales: Zhao, Jianyu, Geng, Chuanqing, Xie, Huimin, Liu, Fei
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9821317/
https://www.ncbi.nlm.nih.gov/pubmed/36614384
http://dx.doi.org/10.3390/ma16010047
_version_ 1784865667921477632
author Zhao, Jianyu
Geng, Chuanqing
Xie, Huimin
Liu, Fei
author_facet Zhao, Jianyu
Geng, Chuanqing
Xie, Huimin
Liu, Fei
author_sort Zhao, Jianyu
collection PubMed
description The fatigue damage assessment of laser-repaired components is critical to their service safety. However, since laser repairing is an advanced green remanufacturing technology, the current research on its fatigue mechanical behavior and fatigue damage evaluation methods is still immature. In addition, the relevant models used for the fatigue damage evaluation can only indicate the fatigue limit of components, which cannot describe the damage accumulation process of the components during the fatigue testing. Therefore, there is an urgent need to develop a fatigue damage evaluation method that can describe the fatigue damage accumulation and evolution to reveal the damage evolution mechanism during the fatigue test. In this study, based on the 3D-DIC technique, new damage parameters, i.e., strain average value and strain standard deviation, are proposed to quantitatively describe the damage status of the nickel-based components during the stress-based fatigue process. Then, based on the new damage parameters, a strain average value/strain standard deviation damage curve method is proposed to describe the damage status evolution of the components during the fatigue testing and evaluate its fatigue damage. For example, in the tensile fatigue test, the strain average value/strain standard deviation damage curves of the substrate component and the laser-repaired component can be divided into two damage stages. In the first damage stage, the damage increases slowly with the increase in the cycle number, whereas in the second damage stage, the damage increases rapidly with the increase in the cycle number. At this time, there is a demarcation point between the first damage stage and second damage stage in the strain average value damage curve and strain standard deviation damage curve. The cycle number of the demarcation point can be used as a reference value for the fatigue failure of the laser-repaired component. In addition, the electron backscatter diffraction (EBSD) technique was used to verify the validity of the evaluation results from the novel damage parameters.
format Online
Article
Text
id pubmed-9821317
institution National Center for Biotechnology Information
language English
publishDate 2022
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-98213172023-01-07 A Novel Parameter for Fatigue Damage Assessment of Laser-Repaired Nickel-Based Alloy Zhao, Jianyu Geng, Chuanqing Xie, Huimin Liu, Fei Materials (Basel) Article The fatigue damage assessment of laser-repaired components is critical to their service safety. However, since laser repairing is an advanced green remanufacturing technology, the current research on its fatigue mechanical behavior and fatigue damage evaluation methods is still immature. In addition, the relevant models used for the fatigue damage evaluation can only indicate the fatigue limit of components, which cannot describe the damage accumulation process of the components during the fatigue testing. Therefore, there is an urgent need to develop a fatigue damage evaluation method that can describe the fatigue damage accumulation and evolution to reveal the damage evolution mechanism during the fatigue test. In this study, based on the 3D-DIC technique, new damage parameters, i.e., strain average value and strain standard deviation, are proposed to quantitatively describe the damage status of the nickel-based components during the stress-based fatigue process. Then, based on the new damage parameters, a strain average value/strain standard deviation damage curve method is proposed to describe the damage status evolution of the components during the fatigue testing and evaluate its fatigue damage. For example, in the tensile fatigue test, the strain average value/strain standard deviation damage curves of the substrate component and the laser-repaired component can be divided into two damage stages. In the first damage stage, the damage increases slowly with the increase in the cycle number, whereas in the second damage stage, the damage increases rapidly with the increase in the cycle number. At this time, there is a demarcation point between the first damage stage and second damage stage in the strain average value damage curve and strain standard deviation damage curve. The cycle number of the demarcation point can be used as a reference value for the fatigue failure of the laser-repaired component. In addition, the electron backscatter diffraction (EBSD) technique was used to verify the validity of the evaluation results from the novel damage parameters. MDPI 2022-12-21 /pmc/articles/PMC9821317/ /pubmed/36614384 http://dx.doi.org/10.3390/ma16010047 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Zhao, Jianyu
Geng, Chuanqing
Xie, Huimin
Liu, Fei
A Novel Parameter for Fatigue Damage Assessment of Laser-Repaired Nickel-Based Alloy
title A Novel Parameter for Fatigue Damage Assessment of Laser-Repaired Nickel-Based Alloy
title_full A Novel Parameter for Fatigue Damage Assessment of Laser-Repaired Nickel-Based Alloy
title_fullStr A Novel Parameter for Fatigue Damage Assessment of Laser-Repaired Nickel-Based Alloy
title_full_unstemmed A Novel Parameter for Fatigue Damage Assessment of Laser-Repaired Nickel-Based Alloy
title_short A Novel Parameter for Fatigue Damage Assessment of Laser-Repaired Nickel-Based Alloy
title_sort novel parameter for fatigue damage assessment of laser-repaired nickel-based alloy
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9821317/
https://www.ncbi.nlm.nih.gov/pubmed/36614384
http://dx.doi.org/10.3390/ma16010047
work_keys_str_mv AT zhaojianyu anovelparameterforfatiguedamageassessmentoflaserrepairednickelbasedalloy
AT gengchuanqing anovelparameterforfatiguedamageassessmentoflaserrepairednickelbasedalloy
AT xiehuimin anovelparameterforfatiguedamageassessmentoflaserrepairednickelbasedalloy
AT liufei anovelparameterforfatiguedamageassessmentoflaserrepairednickelbasedalloy
AT zhaojianyu novelparameterforfatiguedamageassessmentoflaserrepairednickelbasedalloy
AT gengchuanqing novelparameterforfatiguedamageassessmentoflaserrepairednickelbasedalloy
AT xiehuimin novelparameterforfatiguedamageassessmentoflaserrepairednickelbasedalloy
AT liufei novelparameterforfatiguedamageassessmentoflaserrepairednickelbasedalloy