Enhanced High−Temperature Wear Performance of H13 Steel through TiC Incorporation by Laser Metal Deposition
High−temperature wear failure has been a major challenge to die parts. This work provides a comprehensive study on the high−temperature wear performance of a TiC/H13 composite coating prepared by laser metal deposition (LMD). The microstructures of wrought H13 samples, LMD−processed H13 and TiC/H13...
Autores principales: | Lu, Chengqi, Chen, Zhenyu, Yan, Yuqing, Zhuo, Yuhao, Wang, Chuanyang, Jia, Qingbo |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9821728/ https://www.ncbi.nlm.nih.gov/pubmed/36614438 http://dx.doi.org/10.3390/ma16010099 |
Ejemplares similares
-
Effect of Solidification and Hot Rolling Processes on Wear Performance of TiC-Reinforced Wear-Resistant Steel
por: Deng, Xiangtao, et al.
Publicado: (2022) -
The Effect of the Displacement Amplitude on the Fretting Wear of GCr15 Steel with a TiC Coating
por: Liu, Xiaochu, et al.
Publicado: (2022) -
Stellite-6/(WC+TiC) Composite Coatings Produced by Laser Alloying on S355 Steel
por: Bartkowski, Dariusz, et al.
Publicado: (2023) -
The Wear Behavior of the Laser Cladded Ti-Al-Si Composite Coatings on Ti-6Al-4V Alloy with Additional TiC
por: Liu, Ran, et al.
Publicado: (2021) -
The Dry Sliding Wear Properties of Nano-Sized TiC(p)/Al-Cu Composites at Elevated Temperatures
por: Tian, Wei-Si, et al.
Publicado: (2017)