Cargando…
Bond Strength Survival of a Novel Calcium Phosphate-Enriched Orthodontic Self-Etching System after Various Ageing Protocols: An In Vitro Study
OBJECTIVE: This study aimed to evaluate the orthodontic bond strength and enamel-preserving ability of a hydroxyapatite nanoparticles-containingself-etch system following exposure to various ageing methods. MATERIALS AND METHODS: Hydroxyapatite nanoparticles (nHAp) were incorporated into an orthodon...
Autores principales: | , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Hindawi
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9825208/ https://www.ncbi.nlm.nih.gov/pubmed/36624858 http://dx.doi.org/10.1155/2022/3960362 |
_version_ | 1784866588471590912 |
---|---|
author | Garma, Noor M. H. Ibrahim, Ali I. |
author_facet | Garma, Noor M. H. Ibrahim, Ali I. |
author_sort | Garma, Noor M. H. |
collection | PubMed |
description | OBJECTIVE: This study aimed to evaluate the orthodontic bond strength and enamel-preserving ability of a hydroxyapatite nanoparticles-containingself-etch system following exposure to various ageing methods. MATERIALS AND METHODS: Hydroxyapatite nanoparticles (nHAp) were incorporated into an orthodontic self-etch primer (SEP, Transbond™ plus) in three different concentrations (5%, 7%, and 9% wt) and tested versus the plain SEP (control) for shear bond strength (SBS), adhesive remnant index (ARI) scores, and enamel damage in range-finding experiments using premolar teeth. The best-performing formulation was further exposed to the following four artificial ageing methods: initial debonding, 24 h water storage, one-month water storage, and one-month acid challenge. A field-emission scanning electron microscope (FE-SEM) was used to examine the integrity of debonded enamel surfaces and calcium-phosphates (CaPs) reprecipitation. RESULTS: The best-performing formulation (7% nHAp-SEP) resulted in significantly lower SBS (p < 0.001) than the control SEP following the four artificial ageing methods. Nevertheless, it survived the ageing protocols and yielded clinically acceptable SBS with the advantages of leaving minimal adhesive residue, preserving enamel integrity and smoothness, and inducing CaP reprecipitation as confirmed by FE-SEM images. CONCLUSIONS: A newly developed SEP produced adequate orthodontic bond strengths and left unblemished debonded enamel surfaces with minimal remnant adhesive and remineralisation potential, thereby suggesting simpler and safer bonding/debonding procedures. |
format | Online Article Text |
id | pubmed-9825208 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2022 |
publisher | Hindawi |
record_format | MEDLINE/PubMed |
spelling | pubmed-98252082023-01-08 Bond Strength Survival of a Novel Calcium Phosphate-Enriched Orthodontic Self-Etching System after Various Ageing Protocols: An In Vitro Study Garma, Noor M. H. Ibrahim, Ali I. Int J Dent Research Article OBJECTIVE: This study aimed to evaluate the orthodontic bond strength and enamel-preserving ability of a hydroxyapatite nanoparticles-containingself-etch system following exposure to various ageing methods. MATERIALS AND METHODS: Hydroxyapatite nanoparticles (nHAp) were incorporated into an orthodontic self-etch primer (SEP, Transbond™ plus) in three different concentrations (5%, 7%, and 9% wt) and tested versus the plain SEP (control) for shear bond strength (SBS), adhesive remnant index (ARI) scores, and enamel damage in range-finding experiments using premolar teeth. The best-performing formulation was further exposed to the following four artificial ageing methods: initial debonding, 24 h water storage, one-month water storage, and one-month acid challenge. A field-emission scanning electron microscope (FE-SEM) was used to examine the integrity of debonded enamel surfaces and calcium-phosphates (CaPs) reprecipitation. RESULTS: The best-performing formulation (7% nHAp-SEP) resulted in significantly lower SBS (p < 0.001) than the control SEP following the four artificial ageing methods. Nevertheless, it survived the ageing protocols and yielded clinically acceptable SBS with the advantages of leaving minimal adhesive residue, preserving enamel integrity and smoothness, and inducing CaP reprecipitation as confirmed by FE-SEM images. CONCLUSIONS: A newly developed SEP produced adequate orthodontic bond strengths and left unblemished debonded enamel surfaces with minimal remnant adhesive and remineralisation potential, thereby suggesting simpler and safer bonding/debonding procedures. Hindawi 2022-12-31 /pmc/articles/PMC9825208/ /pubmed/36624858 http://dx.doi.org/10.1155/2022/3960362 Text en Copyright © 2022 Noor M. H. Garma and Ali I. Ibrahim. https://creativecommons.org/licenses/by/4.0/This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited. |
spellingShingle | Research Article Garma, Noor M. H. Ibrahim, Ali I. Bond Strength Survival of a Novel Calcium Phosphate-Enriched Orthodontic Self-Etching System after Various Ageing Protocols: An In Vitro Study |
title | Bond Strength Survival of a Novel Calcium Phosphate-Enriched Orthodontic Self-Etching System after Various Ageing Protocols: An In Vitro Study |
title_full | Bond Strength Survival of a Novel Calcium Phosphate-Enriched Orthodontic Self-Etching System after Various Ageing Protocols: An In Vitro Study |
title_fullStr | Bond Strength Survival of a Novel Calcium Phosphate-Enriched Orthodontic Self-Etching System after Various Ageing Protocols: An In Vitro Study |
title_full_unstemmed | Bond Strength Survival of a Novel Calcium Phosphate-Enriched Orthodontic Self-Etching System after Various Ageing Protocols: An In Vitro Study |
title_short | Bond Strength Survival of a Novel Calcium Phosphate-Enriched Orthodontic Self-Etching System after Various Ageing Protocols: An In Vitro Study |
title_sort | bond strength survival of a novel calcium phosphate-enriched orthodontic self-etching system after various ageing protocols: an in vitro study |
topic | Research Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9825208/ https://www.ncbi.nlm.nih.gov/pubmed/36624858 http://dx.doi.org/10.1155/2022/3960362 |
work_keys_str_mv | AT garmanoormh bondstrengthsurvivalofanovelcalciumphosphateenrichedorthodonticselfetchingsystemaftervariousageingprotocolsaninvitrostudy AT ibrahimalii bondstrengthsurvivalofanovelcalciumphosphateenrichedorthodonticselfetchingsystemaftervariousageingprotocolsaninvitrostudy |